Acta Metall Sin  2008, Vol. 44 Issue (7): 786-790     DOI:
Research Articles Current Issue | Archive | Adv Search |
THREE DIMENSIONAL ATOM PROBE CHARACTERAZATION OF MICROSTRUCTURE EVOLUTION AND CARBIDES PRECIPITATION IN THE TEMPERED Nb-V MICROALLOYED STEEL
;;;
上海大学
Cite this article: 

;. THREE DIMENSIONAL ATOM PROBE CHARACTERAZATION OF MICROSTRUCTURE EVOLUTION AND CARBIDES PRECIPITATION IN THE TEMPERED Nb-V MICROALLOYED STEEL. Acta Metall Sin, 2008, 44(7): 786-790 .

Download:  PDF(2825KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Three dimensional atom probe combined with optical microscopy (OM) and transmission electron microscope (TEM) was applied to characterize the carbides precipitation and microstructure evolution in Nb-V microalloyed steel plates quenched and tempered at 500冾600 for 4h. The results indicated that, vanadium and niobium were almost dissolved in matrix with slight segregation of carbon in the as-quenched specimen. A cementite was detected in 450 tempering specimen, as well as V- and Nb-containing carbides with difference sizes and number density in 450,550 and 600 tempering specimens. A maximal strengthen effect of this fine precipitates was obtained at 550 tempering. The carbides started to be coarsened and spheroidzed in 650 tempering specimen.
Key words:  Three Dimensional Atom Probe      Micro-Alloyed Steel      Carbide      Tempered microstructure      
Received:  23 November 2007     
ZTFLH:  TG113.25  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I7/786

[1]Yamazaki K,Koyama K.J Jpn Tech Plast,1994;35:1036
[2]Timokhina I B,Hodgson P D,Ringer S P,Zheng R K, Pereloma E V.Scr Mater,2007;56:601
[3]Rashid M S,Rao B V N.Metall Trans,1982;13A:1679
[4]Hwang G C,Lee S,Yoo J Y,Choo W Y.Mater Sci Eng, 1998;A252:256
[5]Dhua S K,Mukerjee D,Sarma D S.Metall Mater Trans, 2001;32A:2259
[6]Panwer S,Goel D B,Pandey O P,Prasad S.Bull Mater Sci,2006;29:281
[7]Isheim D,Gagliano M S ,Fine M E,Seidman D N.Acta Mater,2006;54:841
[8]Pereloma E V,Timokhina I B,Russell K F,Miller M K. Scr Mater,2006;54:471
[9]Pereloma E V,Shekhter A,Miller M K,Ringer S P.Acta Mater,2004;52:5589
[10]Ping D H,Olmuma M,Hirakawa Y,Kadoya Y,Hono K. Mater Sci Eng,2005;A394:285
[11]Miller M K.Atom Probe Tomography:Analysis at the Atomic Level.New York:Kluwer Academic/Plenum Pub- lishers,2000:11
[12]Weng Y Q.Ultrafine Grained Steel:Microstructure Re- finement Theory and Controlled Technology of Steel.Bei- jing:Metallurgical Industry Press,2003:304 (翁宇庆.超细晶钢:钢的组织细化理论与控制技术.北京:冶金工业出版社,2003:304)
[13]Zhao L C.Principle of Metal Heat Treatment.Harbin: Harbin Institute of Technology Press,1986:201 (赵连城.金属热处理原理.哈尔滨:哈尔滨工业大学出版社,1986:201)
[1] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[2] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[3] HE Shuwen, WANG Minghua, BAI Qin, XIA Shuang, ZHOU Bangxin. Effect of TaC Content on Microstructure and Mechanical Properties of WC-TiC-TaC-Co Cemented Carbide[J]. 金属学报, 2020, 56(7): 1015-1024.
[4] YANG Ke,LIANG Ye,YAN Wei,SHAN Yiyin. Preferential Distribution of Boron and its Effect on Microstructure and Mechanical Properties of (9~12)%Cr Martensitic Heat Resistant Steels[J]. 金属学报, 2020, 56(1): 53-65.
[5] LI Jiarong,XIE Hongji,HAN Mei,LIU Shizhong. High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1195-1203.
[6] Futao DONG,Fei XUE,Yaqiang TIAN,Liansheng CHEN,Linxiu DU,Xianghua LIU. Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. 金属学报, 2019, 55(6): 792-800.
[7] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[8] Tao ZHANG, Wei YAN, Zhuoming XIE, Shu MIAO, Junfeng YANG, Xianping WANG, Qianfeng FANG, Changsong LIU. Recent Progress of Oxide/Carbide Dispersion Strengthened W-Based Materials[J]. 金属学报, 2018, 54(6): 831-843.
[9] Xirong LIU, Kai ZHANG, Shuang XIA, Wenqing LIU, Hui LI. Effects of Triple Junction and Grain Boundary Characters on the Morphology of Carbide Precipitation in Alloy 690[J]. 金属学报, 2018, 54(3): 404-410.
[10] Shenghu CHEN, Lijian RONG. Microstructure Evolution During Solution Treatment and Its Effects on the Properties of Ni-Fe-Cr Alloy[J]. 金属学报, 2018, 54(3): 385-392.
[11] Xiaolin LI, Yang CUI, Baoliang XIAO, Dawei ZHANG, Zhao JIN, Zheng CHENG. Effects of On-Line Rapid Induction Tempering on Pricipitation Strengthening Mechanism of V(C, N) in V-N Microalloyed Steel[J]. 金属学报, 2018, 54(10): 1368-1376.
[12] Yubin DU, Xiaofeng HU, Haichang JIANG, Desheng YAN, Lijian RONG. Effect of Tempering Time on Carbide Evolution and Mechanical Properties in a Fe-Cr-Ni-Mo High-Strength Steel[J]. 金属学报, 2018, 54(1): 11-20.
[13] Bo CHEN, Xianchao HAO, Yingche MA, Xiangdong CHA, Kui LIU. Effects of Nitrogen Addition on Microstructure and Grain Boundary Microchemistry of Inconel Alloy 690[J]. 金属学报, 2017, 53(8): 983-990.
[14] Dawei WANG,Shichao XIU. Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint[J]. 金属学报, 2017, 53(5): 567-574.
[15] Dexin MA, Fu WANG, Xuhui WEN, Dejian SUN, Lin LIU. Influence of MC Carbides on the Formation of γ/γ′ Eutectics in Single Crystal Superalloy CM247LC[J]. 金属学报, 2017, 53(12): 1603-1610.
No Suggested Reading articles found!