| Constitutive Relationship of Hot Deformation of AZ91 Magnesium Alloy |
| ;; |
| 北京科技大学 |
|
Cite this article:
. Constitutive Relationship of Hot Deformation of AZ91 Magnesium Alloy. Acta Metall Sin, 2008, 44(11): 1378-1383 .
|
|
|
Abstract Hot compression deformation of AZ91 magnesium alloy has been performed on Gleeble-1500 under conditions of strain rates of 0.001~1s-1 and deformation temperatures of 250~400℃,the flow stresses in different deformation conditions are investigated. The results show that the flow stress is significantly affected by both deformation temperature and strain rate,the flow stress decreases with the deformation temperature increasing and strain rate decreasing. The relations of the deformation activation energy and stress exponent with strain are obtained using the hyperbolic-sine mathematics model,and the hot deformation constitutive relationship being established. Comparing with experimental results,it is proved that the model reflects the real feature of the deformation of AZ91 alloy.
|
|
Received: 26 March 2008
|
|
|
[1]Mordike B L,Ebert T.Mater Sci Eng,2001;A302:37 [2]Friedrich H,Schumann S.J Mater Process Technol,2001; 117:276 [3]Matucha K H.In:Cahn R W,Hassen P,Kramer E J, eds.;translated by Ding D Y,et al.,Materials Science and Technology:A Comprehensive Treatment,Vol.8:Struc- ture and Properties of Nonferrous Alloys.Beijing:Science Press,1999:105 (Matucha K H.见:Cahn R W,Hassen P,Kramer E J,主编;丁道云,等,译.材料科学与技术丛书,第8卷:非铁合金的结构与性能.北京:科学出版社,1999:105) [4]Takuda H,Fujimoto H,Hatta N.J Mater Process Technol, 1998;80-81:513 [5]Wang L Y,Fan Y G,Huang G J,Huang Y S.Trans Non- ferrous Met Soc China,2003;13:335 [6]Galiyev A,Kaibyshev R,Gottstein G.Acta Mater,2001; 49:1199 [7]Guo Q,Yan H G,Chen Z H,Zhang H.Chin J Nonferrous Met,2005;15:900 (郭强,严红革,陈振华,张辉.中国有色金属学报,2005;15:900) [8]Mwembela A,Konopleva E B,Mcqueen H J.Scr Mater, 1997;37:1789 [9]Galiyev A,Kaibyshev R,Sakai T.Mater Sci Forum,2003; 419-422:509 [10]Tan J C,Tan M J.Mater Sci Eng,2003;A339:124 [11]Poirier J P;translated by Guan D L.Plastic Deforma- tion of Crystal at Elevated Temperature.Dalian:Dalian university of Technology Press,1989:56 (Poirier J P,著;关德林,译.晶体的高温塑性变形.大连:大连理工大学出版社,1989:56) [12]Mcqueen H J,Ryan N D.Mater Sci Eng,2002;A322:43 [13]Gronostajski Z J.J Mater Process Technol,1998;78:84 [14]Imbert C A C,Mcqueen H J.Mater Sci Eng,2001;A313: 88 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|