Abstract According to Norton creep constitutive equation and different creep parameters of welding material, heat-affected zone material and parent material, welding residual stress, post weld heat treatment(PWHT) residual stress and creep under inner pressure and PWHT residual stress of the welded joint of P91 steel high temperature piping were analyzed by ABAQUS finite element code. The distribution of welding residual stress and PWHT residual stress was obtained. Creep strain distribution after 100,000 hours and dangerous position of the welded joint were predicted. The results show the higher welding residual stress is in the welded joint for the piping wall thickness and constraints. And the welding residual stress can be reduced effectively by the method of PWHT. But, because of the existence of PWHT residual stress, the creep strain is also influenced by the PWHT residual stress. The stress can not be neglected in the strength design of high temperature piping. And much higher creep strain is in the edge between welding seam and heat-affected zone. The presente work provides a reference for the design and predicting maintenance for high temperature piping.
|
|
Received: 27 January 2008
|
|
|
[1]Yang F,Zhang Y L,Ren Y N,Li W M.New Heat Resistant Steel Welding.Beijing:China Electric Power Press,2006:1 (杨富,章应霖,任永宁,李为民.新型耐热钢焊接.北京:中国电力出版社,2006:1) [2]Jones D R H.Eng Failure Anal,2004;11:873 [3]Ray A K,Tiwari Y N,Roy P K,Chaudhuri S,Bose S C,Ghosh R N,Whittenberger J D.Mater Sci Eng,2007; A454-455:679 [4]Jeong C S,Bae S Y,Ki D H,Watanabe K,Lim B S.Mater Sci Eng,2007;A448-451:155 [5]Hyde T H,Becker A A,Sun W,Williams J A.Int J Press Vessels Piping,2005;82:509 [6]Hyde T H,Luo R,Becker A A.Int J Press Vessels Piping, 2005;82:625 [7]Hyde T H,Becker A A,Sun W,Williams J A.Int J Press Vessels Piping,2006,83:853 [8]Yang W Y,Li Z W.Acta Metall Sin,1999;35:721 (畅王玥,李志文.金属学报,1999;35:721) [9]Zhang G D,Zhou C Y.Trans China Weld Inst,2007; 28(8):99 (张国栋,周昌玉.焊接学报,2007;28(8):99) [10]HKS Inc.Abaqus User's Manual(Version 6.2).USA: Providence,RI,2000:593 [11]Yang C H,Hu A Z.Jiangxi Electr Power,2005;29(3):21 (杨初惠.胡安中.江西电力,2005,29(3):21) [12]Teng T L,Lin C C.Int J Press Vessels Piping,1998;75: 857 [13]Lu A L,Shi Q Y,Zhao H Y,Wu A P,Cai Z P,Wang P. China Mech Eng,2000;11:201 (鹿安理,史清宇,赵海燕,吴爱萍,蔡志鹏.王鹏.中国机械工程,2000;11:201) [14]Yaghi A H,Hyde T H,Backer A A,Williams J A,Sun W. J Mater Process Technol,2005;167:480 [15]Hyde T H,Backer A A,Sun W,Yaghi A,Williams J A, Concari S.In:Silva J F,Meguid S A ads.,5th Int Conf on Mechanics and Materials in Design,Porto-Portugal: University of Porto,2006:1 [16]Ying R C.Welding Theory and Metallic Material Weld- ing.Beijing:China Machine Press,2000:7 (英若采.熔焊原理及金属材料焊接.北京:机械工业出版社,2000:7) [17]Zhang G D,Zhou C Y.Trans China Weld Inst,2006; 27(12):85 (张国栋.周昌玉.焊接学报,2006;27(12):85) [18]Hyde T H,Sun W,Becker A A.Int J Press Vessels Piping, 2001;78:765 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|