| MICROSTRUCTURE AND MAGNETIC PROPERTIES OF Fe-49%Sn HYPERMONOTECTIC ALLOYS IMPOSED BY A HIGH MAGNETIC FIELD |
| ZUO Xiao-Wei;Wang Engang Wang;Huan HAN;Lin Zhang;Jicheng He |
| 东北大学 材料电磁过程研究教育部重点实验室 |
|
Cite this article:
ZUO Xiao-Wei; Wang Engang Wang; Huan HAN; Lin Zhang; Jicheng He. MICROSTRUCTURE AND MAGNETIC PROPERTIES OF Fe-49%Sn HYPERMONOTECTIC ALLOYS IMPOSED BY A HIGH MAGNETIC FIELD. Acta Metall Sin, 2008, 44(10): 1219-1223 .
|
|
|
Abstract The effect of a high magnetic field (HMF) on solidification microstructure and magnetic properties of Fe-49%Sn hypermonotectic alloys have been studied. It was showed that the morphologies of Fe-rich dendrites could be changed obviously and then magnetic properties were induced to improve. The morphologies of Fe-rich without HMF were dendrites in random and partially cellular structures. The alignment and preferential growth of Fe-rich dendrites paralleled to the applied field occurred with 10T. The primary dendrite arms of Fe-rich phase could be induced to align along [001] direction. The secondary dendrites were broken to fragments and even disappeared. Microstructure evolution and theoretical analysis were proposed to explain these results, which were in terms of magnetic crystalline anisotropy and preferential growth of dendrites. The aligned structures caused the increased magnetic properties such as the maximum magnetic permeability, remanent magnetization and magnetic crystalline anisotropy energy.
|
|
Received: 29 March 2008
|
|
|
[1]Predel B,Ratke L,Fredriksson H.In:Walter H U ed.,A European Perspective:Fluid Sciences and Materials Sci- ence in Space.Berlin:Springer-Verlag,1987:517 [2]Zhang X H,Ruan Y,Wang W L,Wei B B.Sci China, 2007;50G:491 [3]Liu X R,Lu X Y,Wei B B.Sci China,2004;47E:409 [4]He J,Zhao J Z,Wang X F,Zhang Q X,Li H L,Chen G Y.Acta Metall Sin,2007;43:567 (何杰,赵九洲,王晓峰.张钦霞,李海丽,陈桂云.金属学报,2007;43:567) [5]Liu X R,Wang N,Wei B B.Acta Phys Sin,2005;54:1671 (刘向荣,王楠,魏炳波.物理学报,2005;54:1671) [6]Xu J F,Wei B B.Acta Phys Sin,2004;53:1909 (徐锦锋,魏炳波.物理学报,2004;53:1909) [7]Yasuda H,Ohnaka I,Dhindaw B K,Takezawa N, Tamayama T,Fujimoto S,Tsuchiyama A,Nakano T,Ue- sugi K.Trans Indian Inst Metals,2005;58:625 [8]Andrews J B,Hayes L J,Arikawa Y,O'Dell J S,Cheney A B.Mater Sci Forum,1996;215-216:59 [9]St(?)cker C,Ratke L.Mater Sci Forum,2000;329:203 [10]Asai S.J Jpn Inst Metals,1997;61:1271 [11]De Rango P,Lees M,Lejay P,Sulpice A,Tournier R,In- gold M,Germi P,Pernet M.Nature,1991;349:770 [12]Sassa K,Morikawa H,Asai S.J Jpn Inst Metals,1997;61: 1283 [13]Jia G Q,Zhang J C,Liu Y S,Zhang X Y,Ren Z M,Cao S X,Li X,Deng K.Acta Phys Sin,2005;54:1126 (贾广强,张金仓,刘永生,张晓勇,任忠鸣,曹世勋,李喜,邓康.物理学报,2005;54:1126) [14]Yasuda H,Ohnaka I,Yamamoto Y,Tokieda K,Kishio K. Mater Trans,2003;44:2207 [15]Asai S,Sassa K,Tahashi M.Sci Technol Adv Mater,2003; 4:455 [16]Baker H,Okamoto H.Alloy Phase Diagrams.Materials Park,Ohio:ASM International,1992:2-203 [17]Giefers H,Nicol M.J Alloy Compd,2006;422:132 [18]Cullity B D.Introduction to Magnetic Materials.Read- ing,Massachusetts:Addison-Wesley,1972:208 [19]Morikawa H,Sassa K,Asai S.Mater Trans,JIM,1998; 39:814 [20]Flemings M C.Solidification Processing.New York: McGraw-Hill,1974:159 [21]Kurz W,Fisher D J.Fundamentals of Solidification.4th Ed.,Switzerland:Trans Tech Publications,1998:69 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|