Abstract The effects of B content on the columnar structures of unidirectionally solidified Ti-46Al and Ti-46Al-5Nb alloys were investigated in the paper. The results show that, with B addition, the columnar structures of Ti-46Al and Ti-46Al-5Nb alloys are refined. The effect of B addition on the columnar structure refinement of Ti-46Al-5Nb alloy is greater than that of Ti-46Al alloy. This is resulted from two reasons. (1) The effects of Nb addition on the columnar structure refinement of Ti-46Al alloy. (2) In Ti-46Al alloy the boride fraction is increased because the solubility of B element was decreased with Nb addition.
|
|
Received: 26 February 2008
|
|
|
[1]Dimiduk D M.Mater Sci Eng,1999;A263:281 [2]Jung I S,Jang H S,Oh M H,Lee J H,Wee D M.Mater Sci Eng,2002;A329-331:13 [3]Yamaguchi M,Johnson D R,Lee H N,Inui H.Inter- metallics,2000;8:511 [4]Lu Y H,Zhang Y G,Qiao L J,Wang Y B,Chen C Q,Chu W Y.Acta Metall Sin,1999;35:1233 (陆永浩,张永刚,乔利杰,王燕斌,陈昌麒,褚武扬.金属学报,1999;35:1233) [5]Zhang J,Zhang Z H,Zou D X,Zhong Z Y.Acta Metall Sin,1996;32:1044 (张继,张志宏,邹敦叙,仲增墉.金属学报,1996;32:1044) [6]Hu D.Intermetallics,2001;9:1037 [7]Dong L M,Cui Y Y,Yang R.Acta Metall Sin,2002;38: 643 (董利民,崔玉友,杨锐.金属学报,2002;38:643) [8]Cheng T T.Intermetallics,2000;8:29 [9]Rao G B,Liu K,Han E H,Ke W.Chin d Nonferrous Metals,2004;14(Suppl.1):265 (饶光斌,刘奎,韩恩厚,柯伟.中国有色金属学报,2004;14(专辑1):265) [10]Larson D J,Liu C T,Miller M K.Mater Sci Eng,1997; A239-240:220 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|