| NUMERICAL SIMULATION OF ELECTROMAGNETISM PARAMETERS AND STRUCTURE PARAMETERS IN TWO-STAGE SLIT-LESS MOLD |
| Bai-Gang JIN |
| 东北大学材料电磁过程教育部重点实验室 |
|
Cite this article:
Bai-Gang JIN. NUMERICAL SIMULATION OF ELECTROMAGNETISM PARAMETERS AND STRUCTURE PARAMETERS IN TWO-STAGE SLIT-LESS MOLD. Acta Metall Sin, 2007, 43(4): 427-432 .
|
|
|
Abstract Numerical simulation and orthogonal experiment had been conducted to study the magnetic field distribution in the two-stage soft contact EMCC (electromagnetic continuous casting) mold of round billets. The effects of some factors such as the thickness of mold wall, the resistivity of mold upside part, electrical frequency and coil current intensity to the penetration of magnetic field in two-stage mold were investigated. The magnetic flux density is decreased with the electrical frequency and thickness of mold increasing, but increased with the resistivity of upside mold and coil current intensity increasing. The order of factors affecting the penetration of magnetic field in two-stage mold is electrical frequency>mold upside resistivity>coil current intensity>mold wall thickness. By dimensionless analysis, the relation equation between magnetic flux density and four parameters was given: B/(μ0I/d)= 4.36×109(ρ/If)0.89. Finally, the perfect parameters of two-stage mold used in EMCC are obtained: the thickness of mold wall is 5 mm,the resistivity of mold upside part is 8.8×10-7 Ω•m,coil current intensity is 2000 A, the supply frequency is above 2000 Hz.
|
|
Received: 10 August 2006
|
|
|
[1]Asai S.Tetsu Hagané,1989;75:32 (浅井滋生.铁钢,1989;75:32) [2]Toh T,Takeuchi E,Hojo M,Kawai H,Matsumura S.ISIJ Int,1997;37:1112 [3]Tanaka T,Kurita K,Kuroda A.ISIJ Int,1991;31:350 [4]Yu G W,Jia G L,Wang E G,He J C.Acta Metall Sin, 2002;38:208 (于光伟,贾光霖,王恩刚,赫冀成.金属学报,2002;38:208) [5]Iwai K,Sassa K,Asai S.Electromagnetic Forces and Ap- plications.Amsterdam:Elsevier Science Publishers,1992: 263 [6]Park J,Jeong H,Kim H,Kim J.ISIJ Int,2002;42:385 [7]Cha P R,Hwang Y S,Oh Y J,Chung S H,Yoon J K. ISIJ Int,1996;36:1157 [8]Fuchigami Y,Suenaga R,Takeuchi E.Japan Pat,JP 3099753,1991 [9]Wang Q,He J C,Wang E G.China Pat,ZL 02132867.6, 2002 (王强,赫冀成,王恩刚.中国专利,ZL 02132867.6,2002) [10]Deng A Y,Jia G L,He J C.Acta Metall Sin(Engl Lett), 2001;14:137 [11]Jin B G,Wang Q,Liu Y,Cui D W,Wu C T,Wang E G, He J C.Chin J Nonferrous Met,2006;16:1931 (金百刚,王强,刘燕,崔大伟,吴成涛,王恩刚,赫冀成.中国有色金属学报,2006;16:1931) [12]Na X Z,Zhang X Z,Gan Y.ISIJ Int,2002;9:974 [13]Liu W Q.Design of Experiments.Beijing:Tsinghua Uni- versity Press,2005:64 (刘文卿.实验设计.北京:清华大学出版社,2005:64) [14]Chen J X.Manual of Continuous Casting.Beijing:Met- allurgical Industry Press,1995:168 (陈家祥.连续铸钢手册.北京:冶金工业出版社,1995:168) [15]Suzuki T,Mori H.Electr Furn Steel,1999;70:133 (铃木寿穗,森広司.电气制钢,1999;70:133) [16]Jia F,Jin J Z,Zhang X G,Li Y M,Cao Z Q.J Dalian Univ Technol,2003;43:305 [17]Cha P R,Hwang Y S,Nam H S,Chung S H,Yoon J K. ISIJ Int,1998;38:403 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|