Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (4): 388-392     DOI:
Research Articles Current Issue | Archive | Adv Search |
OXIDATION RESISTANCE OF COPPER PARTICLES MODIFIED WITH MANNICH BASES
石家庄军械工程学院三系
Cite this article: 

. OXIDATION RESISTANCE OF COPPER PARTICLES MODIFIED WITH MANNICH BASES. Acta Metall Sin, 2007, 43(4): 388-392 .

Download:  PDF(463KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Oxidation resistance of copper particles modified with one king of mannich base was studied. Anti-corrosion properties were tested by etching copper particles in acid medium, and the results showed that the corrosion of copper particles was effectively inhabited by modification with the mannich base. On the basis of TG-DTA thermal analysis, we found the original copper particles were oxidized at 200 degrees centigrade, while the treated copper particles were oxidized at 300 degrees, 100 degrees higher than the original ones. XPS analysis showed the mannich base improved the oxidation resistance of copper particles by coordinating with Cu2+ to form protective film on the surface of copper particles. To discover the reaction between the manncih base and copper particles, we tried to obtain the reaction product of the mannich base and copper particles, and furthmore prepared the complex of the manncih base and Cu2+. IR and UV-vis spectrum of the complexes showed that the N atom in the manncih base molecular, instead of O atom was the coordinating atom bonded to Cu2+.
Key words:  copper particles      mannich base      oxidation resistance      complex      
Received:  02 June 2006     
ZTFLH:  TG174.42  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I4/388

[1]Syed A S,Satheesh A,Ramu K K.Ramu S,Venkatachari G.Prog Org Coat,2006;55:1
[2]Cheng K B,Ramakrishna S,Lee K C.Composites,2000; 31A:1039
[3]Kim J,Satoh M,Iwasaki T.Mater Sci Eng,2003;A342: 258
[4]Pavlovi G,Pavlovi L J,Doroslovaki I D.Hydrometallurgy, 2004;73:155
[5]Xu X R,Luo X J,Zhuang H R,Li W L,Zhang B L.Mater Lett,2003;57:3987
[6]Zhao B,Liu Z J,Zhang Z T.Hu L M.J Solid State Chem, 1997;130:157
[7]Du S G,Yan J,Zhang T L.Electron Components Mater, 2004;23(12):40 (杜仕国,闫军,张同来.电子元件与材料,2004;23(12): 40)
[8]Yan J,Cui H P,Du S G.J Mater Prot,2003;36:30 (闫军,崔海萍,杜仕国.材料保护,2003;36:30)
[9]Vuorinen E,Ngobent P,Vander G H.Br Corros J,1994; 29:120
[10]Wang J,Zhang W.Spec Petrochem,2001;18(4):19 (王江,张卫.精细石油化工,2001;18(4):19)
[11]Peissker E.Met Powder Rep,1991;46:20
[12]Cao C N.Corrosion Electrochemistry.Beijing:Chemical Industry Press,1994:131(曹楚南.腐蚀电化学,北京:化学工业出版社,1994:131)
[13]Zhai J K.High Temperature Corrosion of Metal.Beijing: Beijing University of Aeronautics and Astronautics Press, 1994:31 (翟金坤.金属高温腐蚀.北京:北京航空航天大学出版社,1994: 31)
[14]Otmacic H,Tclcgdi J.J Appl Electrochem,2004;34:545
[15]Wang G H,Harrison A.J Colloid Interface Sci,1999;217: 203
[16]Zhu L L,Teng Q W,Wu S.Chin J Struct Chem,2006; 25:143
[17]David H.Modern Analytiscal Chemistry.New York: McGraw-Hill Co.Inc.,2000:388
[18]Torreggiani A,Tamba M,Trinchero A,Bonora S.J Mol Struct,2005;746:759
[1] ZHAO Xiaofeng, LI Ling, ZHANG Han, LU Jie. Research Progress in High-Entropy Alloy Bond Coat Material for Thermal Barrier Coatings[J]. 金属学报, 2022, 58(4): 503-512.
[2] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[3] LI Tianxin, LU Yiping, CAO Zhiqiang, WANG Tongmin, LI Tingju. Opportunity and Challenge of Refractory High-Entropy Alloys in the Field of Reactor Structural Materials[J]. 金属学报, 2021, 57(1): 42-54.
[4] GONG Shengkai, SHANG Yong, ZHANG Ji, GUO Xiping, LIN Junpin, ZHAO Xihong. Application and Research of Typical Intermetallics-Based High Temperature Structural Materials in China[J]. 金属学报, 2019, 55(9): 1067-1076.
[5] Bin LI, Xiaohui LIN, Rui LI, Guojun ZHANG, Laiping LI, Pingxiang ZHANG. High-Temperature Oxidation Resistance of Mo-Si-B Alloys with Different B Contents[J]. 金属学报, 2018, 54(12): 1792-1800.
[6] Hongxi LIU,Zhengxue LI,Xiaowei ZHANG,Jun TAN,Yehua JIANG. Effect of Heat Treatment on High-Temperature Oxidation Resistance of High Niobium Ti-Al Intermetallic Coating Fabricated by Laser In Situ Synthesis on Titanium Alloy[J]. 金属学报, 2017, 53(2): 201-210.
[7] Haigen ZHAO,Shusuo LI,Yanling PEI,Shengkai GONG,Huibin XU. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ni3Al-BASED SINGLE CRYSTSAL ALLOY IC21[J]. 金属学报, 2015, 51(10): 1279-1287.
[8] ZHOU Xiaowei SHEN Yifu GU Dongdong. MICROSTRUCTURE AND HIGH TEMPERATURE OXIDATION RESISTANCE OF NANOCRYSTALLINE Ni–CeO2 COMPOSITE COATINGS DEPOSITED BY DOUBLE–PULSED ELECTRO DEPOSITION[J]. 金属学报, 2012, 48(8): 957-964.
[9] MA Yue SU Hang PAN Tao YU Yinhong YANG Caifu ZHANG Yongquan PENG Yun. STUDY OF COMPLEX DUCTILE INCLUSIONS CONTROLLING IN MEDIUM-HIGH CARBON STEELS[J]. 金属学报, 2012, 48(11): 1321-1328.
[10] HU Zhiyong YANG Chengwei JIANG Min YANG Guangwei WANG Wanjun WANG Xinhua . IN SITU OBSERVATION OF INTRAGRANULAR ACICULAR FERRITE NUCLEATED ON COMPLEX TITANIUM–CONTAINING INCLUSIONS IN TITANIUM DEOXIDIZED STEEL[J]. 金属学报, 2011, 47(8): 971-977.
[11] SHU Wei WANG Xuemin LI Shurui HE Xinlai. NUCLEATION AND GROWTH OF INTRAGRANULAR ACICULAR FERRITE AND ITS EFFECT ON GRAIN REFINEMENT OF THE HEAT-AFFECTED-ZONE[J]. 金属学报, 2011, 47(4): 435-441.
[12] LI Yuling MA Weimin WEN Lei WEN Qiang YUAN Xiaoyu. INFLUENCES OF PREPARATION PARAMETERS ON MORPHOLOGY AND PHOTOLUMINESCENCE PROPERTY OF BaZrO3:Ce NANO-POWDERS[J]. 金属学报, 2011, 47(1): 95-101.
[13] HOU Dangshe; LI Kezhi; LI Hejun; FU Qiangang; WEI Jian; HE Yonggang. Study on the SiC-TaSi2/MoSi2 Multilayer Oxidation Protective Coating for Carbon/Carbon composites[J]. 金属学报, 2008, 44(3): 331-335 .
[14] . MICROWAVE ABSORBING CAPABILITY OF FeSiAlCr NANO-CRYSTALLINE FLAKES[J]. 金属学报, 2006, 42(3): 321-324 .
[15] WU Yingna; KE Peiling; SUN Chao; HUA Weigang; WANG Fuhui; WEN Lishi. NiCrAlY/NiAl/ZrO2-Y2O3 Thermal Barrier Coatings Obtained by Detonation Spraying[J]. 金属学报, 2004, 40(5): 541-545 .
No Suggested Reading articles found!