Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (10): 1059-1064     DOI:
Research Articles Current Issue | Archive | Adv Search |
Cite this article: 

. . Acta Metall Sin, 2007, 43(10): 1059-1064 .

Download:  PDF(522KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  ZrO2-SiC composite was synthesized from zirconite and carbon black by carbothermal reduction reaction in argon atmosphere, and it was as the additive to apply in Al2O3-C refractories. The effect of the heating temperature on the synthesis and the addition of the synthesized composite on the oxidation resistance of the Al2O3-C refractories were studied. The research results showed that the synthesized composite could be easily obtained by heating the mixture of zirconite and carbon black at 1600 ℃ for 4 h in argon atmosphere, and the oxidation resistance of the Al2O3-C refractories could be obviously improved by adding the synthesized ZrO2-SiC composite.
Key words:  ZrO2-SiC composite      synthesis      carbothermal reduction      oxidization resistance      Al2O3-C refractory      
Received:  16 January 2007     
ZTFLH:  TF065.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I10/1059

[1]Chan C F,Argent B B,Lee W E.Calphad,2003;27:115
[2]Yamaguchi A.Taikabutsu Overseas,1984;4(3):14
[3]Sun Y,Yu J K.Chin Refract,2007;16(Suppl.):177
[4]Yu J K,Hiragushi K.Taikabutsu Overseas,1998;19(2): 11
[5]Yu J K,Dai W B,Dai S P.,1 Northeast Univ(Nat Sci), 2003;24:824 (于景坤,戴文斌,戴淑平.东北大学学报(自然科学版),2003;24:824)
[6]Chen M,Song Y L,Yu J K.Chin Refract,2007; 16(Suppl.):134
[7]Chen W W,Zou Z S,Wang T M.Acta Metall Sin,1997; 33:643 (陈卫武,邹宗树,王天明.金属学报,1997;33:643)
[8]Ma B Y,Tan C,Yu J K.Chin Refract,2007;16(Suppl.): 158
[9]Liang Y J,Che Y C.Handbook of Thermodynamics Data in Inorganic.Shenyang:Northeastern University Press, 1993:449 (梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:449)
[10]Chen Z Y.Chemical Thermodynamics of Refractories. Beijing:Metallurgical Industry Press,2005:539 (陈肇友.化学热力学与耐火材料.北京:冶金工业出版社,2005:539)
[1] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[2] CHEN Fei, QIU Pengcheng, LIU Yang, SUN Bingbing, ZHAO Haisheng, SHEN Qiang. Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. 金属学报, 2023, 59(1): 180-190.
[3] ZHAO Lei, WANG Hui, YANG Lixia, CHEN Xuebin, LANG Runqiu, HE Linfeng, CHEN Dongfeng, WANG Haizhou. First Exploration of Hot Isostatic Pressing High-Throughput Synthesis on Fe-Co-Ni Combinatorial Alloy[J]. 金属学报, 2021, 57(12): 1627-1636.
[4] ZHANG Xia, SONG Yang, WANG Yu, JI Luhe, YANG Mei, MENG Hao. Ultrasonic Blending Synthesis of Ni(HNCN)2/BiVO4 Composite Visible-Light Induced Photocatalysts[J]. 金属学报, 2020, 56(11): 1551-1557.
[5] Hongxi LIU,Zhengxue LI,Xiaowei ZHANG,Jun TAN,Yehua JIANG. Effect of Heat Treatment on High-Temperature Oxidation Resistance of High Niobium Ti-Al Intermetallic Coating Fabricated by Laser In Situ Synthesis on Titanium Alloy[J]. 金属学报, 2017, 53(2): 201-210.
[6] HU Na, XUE Lihong, GU Jian, LI Heping, YAN Youwei. OPTIMIZATION OF GRADING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Al13Fe4/Al COM- POSITES IN SITU SYNTHESIZED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2015, 51(2): 216-222.
[7] LU Ke. GRADIENT NANOSTRUCTURED MATERIALS[J]. 金属学报, 2015, 51(1): 1-10.
[8] WANG Ying, ZOU Binglin, CAO Xueqiang. COMBUSTION SYNTHESIS OF TiC-TiB2 PARTICU- LATES LOCALLY REINFORCED STEEL MATRIX COMPOSITES FROM AN Al-Ti-B4C SYSTEM DURING CASTING[J]. 金属学报, 2014, 50(3): 367-372.
[9] ZHU Hongyan, MA Weimin, WEN Lei, GUAN Renguo,MA Lei, WU Nan. SYNTHESIS KINETICS OF (Y, Gd)2O3∶Eu3+ NANO-POWDERS DURING PROCESS OF PREPARATION[J]. 金属学报, 2012, 48(6): 671-677.
[10] ZHANG Xiaowei LIU Hongxi JIANG Yehua WANG Chuanqi. LASER IN SITU SYNTHESIZED TiN/Ti3Al COMPOSITE COATINGS[J]. 金属学报, 2011, 47(8): 1086-1093.
[11] DAI Wenbin WANG Xinli YU Jingkun ZOU Zongshu. PRODUCTION OF MgAlON BY CARBOTHERMAL REDUCTION AND NITRIDATION[J]. 金属学报, 2011, 47(11): 1440-1444.
[12] LIU Linlin LI Shu LIU Yang. ANTI–FRICTION BEHAVIORS OF SEVERAL SYNTHESIZED PERRHENATES[J]. 金属学报, 2010, 46(2): 233-238.
[13] Hai-Chang JIANG. Ni RELEASING BEHAVIOR OF POROUS TiNi SHAPE MEMORY ALLOY[J]. 金属学报, 2008, 44(2): 198-202 .
[14] LingLing Wang. Low-Temperature Combustion Synthesis Of Nanocrystalline Ce1-Xndxo2-X/2 Powders[J]. 金属学报, 2006, 42(5): 511-514 .
[15] Ye Pan. TRIBOLOGICAL PROPERTIES OF COMBUSTION SYNTHESISED Cr-Al(Cr)2O3 CERMETS[J]. 金属学报, 2006, 42(5): 492-496 .
No Suggested Reading articles found!