Cite this article:
. . Acta Metall Sin, 2007, 43(10): 1043-1047 .
|
|
|
Abstract ZnO films have been prepared on glass by sol-gel dip coating. The crystal structure and surface morphology were characterized by X -ray diffractometer and scanning electron microscope, respectively. It could be concluded: solvent with higher boiling point helped to obtain ZnO with stronger preferred orientation; MEA was quite effective in formation of ZnO films with strong orientation, while DEA and TEA were not; pretreatment should be finished before the beginning of the crystallization of ZnO gel film; postreatment at higher temperature induced bigger grain size and stronger preferred orientation at 400 - 500℃.
|
|
Received: 12 February 2007
|
|
|
[1]Nishino J,Kawarada T,Ohisho S,Saitoh H,Maruyama K,Kamata K.J Mater Sci Lett,1997;16:629 [2]Wang R P,King L L H,Sleight A W.J Mater Res,1996; 11:1659 [3]Messaoudi C ,Sayah D,Abdlefdil M.Phys Status Solidi, 1995;151:93 [4]Yoon K H,Choi J W,Lee D H.Thin Solid Film,1997; 302:116 [5]Hu J H,Gordon R G.J Appl Phys,1992;72:5381 [6]Lokhande B J,Patil P S,Uplane M D.Mater Lett,2002; 57:573 [7]Spanhel L,Anderson M.J Am Chem Soc,1991;113:2826 [8]Ohyama M,Sukozuka H,Yoko T.Thin Solid Film,1997; 306:78 [9]Birkholz M,Selle B,Fenske F,Fuhs W.Phys Rev,2003; 68B:205414 [10]Fujimura N,Nishihara T,Goto S,Xu J F,Ito T.J Cryst Growth,1993;130:269 [11]Brinker C J,Scherer W G.Sol-Gel Science:The Physics and Chemistry of Sol-Gel Processing.San Diego:Aca- demic Press,Inc,1990 [12]Scherer W G.J Sol Gel Sci Technol,1997;8:353 [13]Znaidi L,Soler Illia G J A A,Benyahia S,Sanchez C, Kanaev A V.Thin Solid Film,2003;428:257 [14]Spanhel L.J Sol-Gel Sci Technol,2006;39:7 [15]Zhou H M,Yi D Q,Yu Z M,Xiao L R,Li J,Wang B. Acta Metall Sin,2006;42:505 (周宏明,易丹青,余志明,肖来荣,李荐,王斌.金属学报,2006;42:505) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|