Abstract An investigation into the microstructure in directional solidified hypoeutectic Al-4.5Cuwt.%alloys under a longitudinal magnetic field shows that the field has a great influence on the dendritic arrays. The field causes severe distortion in the dendritic array morphology in the mushy zone and disappeared below the eutectic isotherm at lower growth speed R=5µm/s, as opposed to the well-aligned dendritic crystals in the absence of the field; At the growth speed R=50µm/s and a temperature gradient in the liquid of 38K/cm, the alignment structure forms and the crystal direction <111> turns to the direction of the magnetic field, as opposed to the dendrite growth along the crystal direction<100>. It has also been found the field causes the increase of primary dendrite arm spacing at the growth speed R=100µm/s, Above phenomena is analysed on the base of the TEMHD theory and crystal.magnetic anisotropy theory.
[1] Katsuki A, Tokunaga Ft, Watanabe S, Tanimoto Y. Chem Lett, 1996; 25: 607 [2] Tahashi M, Sassa K, Asai S. Mater Trans, 2002; 43: 2813 [3] Fang Q Q, Pang R Y, Zhang S, Dai D S. J Magn Magn Mater, 1998; 188: 241 [4] Shercliff J A. J Fluid Mech, 1979; 91: 231 [5] Lehmann P, Moreau R, Camel D, Bolcato R, Acta Mater, 1998; 46: 4067 [6] Boettinger W J, Biancaniello F S, Coriell S R. Metall Trans, 1981; 12A: 321 [7] Tewari S N, Shah R, Song H. Metall Mater Trans, 1994; 25A: 1535 [8] Wu Q, Ren Z M, Li X, Deng K, Zhong Y B, Ma J P. Prog Nat Sci, 2004; 14: 830(吴琼,任忠鸣,李喜,邓康,钟云波,马娟萍.自然科学进展,2004;14:830) [9] Ma J P, Ren Z M, Deng K, Li X, Wu Q. Prog Nat Sci, 2004; 14: 837(马娟萍,任忠鸣,邓康,李喜,吴琼.自然科学进展,2004;14:837) [10] Callen H B. Phys Rev, 1984; 73: 1349 [11] Cui Z Q. Metallurgy and Heat Treatment. Beijing: China Machine Press, 1994: 10(崔忠圻.金属学与热处理.北京:机械工业出版社,1994:10)