| Effects of Hydrogen on the Microstructure and High Temperature Mechanical Properties of Ti--60 Alloy |
| LI Fang |
| 上海大学材料研究所 |
|
Cite this article:
LI Fang. Effects of Hydrogen on the Microstructure and High Temperature Mechanical Properties of Ti--60 Alloy. Acta Metall Sin, 2006, 42(2): 143-146 .
|
|
|
Abstract The effect of hydrogen charging on the microstructure (α+β)/βtransformation and the mechanical properties of Ti-60 alloy at high temperature have been investigated. The results show that the volume fraction of primaryαand the (α+β)/βtransformation temperature is continuously decreased with increasing hydrogen contents. The result also indicate that the yield strength at high temperature is also continuously decreased with hydrogen concentration, and the minimum yield strength occurs at a concentration which corresponds to the (α+β)/βtransition and that further increase in yield strength is due to the hardening effect of hydrogen addition in the βphase.
|
|
Received: 27 May 2005
|
|
|
[1] Han M C. Aerosp Mater Technol, 1999; (1): 23(韩明臣.宇航材料工艺,1999;(1):23) [2] Ilyin A A, Polkin I S, Moamonov A M, Nosov V K. In: Blenkinsop P A, Evans W J, Flower H M, eds., Titanium'95: Science and Technology, London: Institute of Materials, 1996: 2462 [3] Costa J E, Williams T C, Thompson A W. Metall Trans, 1987; 18A: 1421 [4] Hou H L, Li Z Q, Wang Y J, Guan Q. Chin J Nonferrous Met, 2003; 13: 533 (侯红亮,李志强,王亚军,关桥.中国有色金属学报,2003;13:533) [5] Senkov O N, Froes F H. Int J Energy, 1999; 24: 565 [6] Murzinova M A, Salishchev G A, Afonichev D D. Int J Energy, 2002; 27: 775 [7] Kerr W R, Smith P R, Rosenblum M E, Gurney F J, Mahajan Y R, Bidwell L R. In: Kimura H, Izumi O, eds., Titanium 80: Science and Technology. Warrendale: TMSAIME, 1980: 2477 [8] Lai Z H. In: Sun W C, Cui Z P, eds., Proc 7th National Conf on Titanium and Titanium Alloys, Changsha: Central South University of Technology Press, 1991: 266 (赖祖涵.见:孙文川,崔祝屏主编,第七届全国钛及钛合金学术交流会文集,长沙:中南工业大学出版社,1991:266) [9] Fang T Y, Wang W H. Mater Chem Phys, 1998; 56: 35 [10] Yang K, Edmonds D V. Scr Metall Mater, 1993; 28: 71 [11] Senkov O N, Jonas J J. Metall Mater Trans, 1996; 27A: 1869G |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|