Abstract Grain boundary hardening and slip transmission across grain boundary are two
important aspects in deformation of materials. Using depth--sensing
indentation, a pop--in phenomenon induced by grain boundaries
has been observed in polycrystalline niobium. This
phenomenon is about a sudden displacement jump observed
near a grain boundary segment at a larger force than the initial
elasto--plastic pop--in, which is observed
not to be affected by grain boundary. The experimental
results show that this pop--in
effect has a close relationship with misorientations of the grain
boundary. Further studies found that no evident change of grain
boundary hardness was observed even though there existed
grain boundary pop--in.
|
|
Received: 11 October 2004
|
|
|
[1] Aust K T, Hanneman R E, Niessen P, Westbrook J H. Acta Metall, 1968; 16: 291 [2] Watanabe T, Kitamura S, Karashima S. Acta Metall, 1980; 28: 455 [3] Harris L B, Howes V R, Cutmore N G. J Amer Ceramic Soc, 1982; 65: 35 [4] Chou Y T, Cai B C, Romig Jr A D, Lin L S. Phill Mag, 1983; 47A: 363 [5] Zhou Z Q, Chou Y T. J Less Common Met, 1985; 114: 323 [6] Wyrzykowski J W, Grabski M W. Philos Mag, 1986; 53A: 505 [7] Lee C S, Han G W, Smallman R E, Feng D, Lai J K L. Acta Mater, 1999; 47: 1823 [8] Wo P C, Ngan A H W. J Mater Res, 2004; 19: 189 [9] Gerberich W W, Nelson J C, Lilleodden E T, Anderson P, Wyrobek J T. Acta Mater, 1996; 44: 3585 [10] Bahr D F, Kramer D E, Gerberich W W. Acta Mater, 1998; 46: 3605 [11] Corcoran S G, Colton R J. Phys Rev, 1997; 55B: R16057 [12] Kramer D, Huang H, Kriese M, Robach J, Nelson J, Wright A, Bahr D, Gerberich W W. Acta Mater, 1999; 47: 333 [13] Chiu Y L, Ngan A H W. Acta Mater, 2002; 50: 2677 [14] Zielinski W, Huang H, Gerberich W W. J Mater Res, 1993; 8: 1300 [15] Shen Z, Wagoner RH, Clark WAT. Acta Metall, 1988; 36: 3231 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|