| Kinetics of Structure Evolution During Deformation Enhanced Transformation in a Low Carbon Steel SS400 |
| QI Junjie; YANG Wangyue; SUN Zuqing; ZHANG Xiaozhong; DONG Zhifeng |
| Department of Materials Science and Engineering; Tsinghua University; Beijing 100084; Department of Materials Science & Engineering; University of Science & Technology Beijing; Beijing 100083 |
|
Cite this article:
QI Junjie; YANG Wangyue; SUN Zuqing; ZHANG Xiaozhong; DONG Zhifeng. Kinetics of Structure Evolution During Deformation Enhanced Transformation in a Low Carbon Steel SS400. Acta Metall Sin, 2005, 41(6): 605-610 .
|
|
|
Abstract Quantitative characterization of microstructural evolution during
deformation enhanced transformation in a low carbon steel SS400
was investigated on a Gleeble 1500 machine. General conclusions
of the austenite transformation kinetics were formulated. It was
shown that the transformation process can be divided into three stages
according to the characteristics of transformation kinetics: The
kinetics equations of two early stages fitted well in with the
J-M-A equation. The kinetics of the first stage obeys Cahn's
site saturation mechanism, the kinetics parameter n=4 which indicates
the ferrite nucleates at austenite grain boundaries and triple points.
Kinetics of the second stage doesn't obey Cahn's
theory, the kinetics parameter n=1.0-1.5, corresponding to ferrite
nucleating repeatedly at the high stored energy areas in front of
the ferrite/austenite interface. The kinetics doesn't obey the
J-M-A equation anymore in the final stage, and only few nucleation
sites left at this moment. Deformation promotes the growth of ferrite
grains, the growing rate of ferrite in the early stage of DEFT was calculated.
|
|
Received: 09 October 2004
|
|
|
[1]Mintz B,Abu-Shosha R,Shaker M.Mater Sci Technol,1993;9:907 [2]Mintz B,Lewis H,Jonas J J.Mater Sci Technol,1997;13:379 [3]Hurley P J,Hodgson P D,Muddle B C.Scr Mater,1999;40:433 [4]Hurley P J,Hodgson P D.Mater Sci Eng,2001;A302:206 [5]Hickson M R,Hurley P J,Gibbs R K,Kelly G L,Hodgson P D.Metall Mater Trans,2002;33A:1019 [6]Yang W Y,Hu A M,Qi J J,Sun Z Q.Acta Metall Sin,2000;36:1192 (杨王明,胡安民,齐俊杰,孙祖庆.金属学报,2000;36:1192) [7]Cahn J W.Acta Metall,1956;9:449 [8]Khlestov V M,Konopleva E V,Mcqueen H J.Can Metall Q,1998;37:75 [9]Li J,Sun F Y.Acta Metall Sin,1990;26:A378 (李箭,孙福玉.金属学报,1990;26:A378) [10]Yang P,Fu Y Y,Cui F E,Sun Z Q.Acta Metall Sm,2001;37:617 (杨平,傅云义,崔凤娥,孙祖庆.金属学报,2001;37:617) [11]Tamura Imao.Iron Steel,1985;20(1):64 (田村今男 钢铁,1985;20(1):64) [12]Qi J J,Yang W Y,Sun Z Q.Acta Metall Sm,2002;38:897 (齐俊杰,杨王玥,孙祖庆.金属学报,2002;38:897) |