| TEM observation of annealing microstructure of deformed Al-Mg-Sc-Zr alloy |
| ZHAO Weitao; YAN Desheng; RONG Lijian |
| Institute of Metal Research; The Chinese Academy of Sciences |
|
Cite this article:
ZHAO Weitao; YAN Desheng; RONG Lijian. TEM observation of annealing microstructure of deformed Al-Mg-Sc-Zr alloy. Acta Metall Sin, 2005, 41(11): 1150-1154 .
|
|
|
Abstract Al-6Mg-0.4Mn-0.2Sc-0.1Zr-0.1Cr(mass fraction, %) alloy was prepared by vacuum induction melting, and the microstructures and mechanical properties of cold worked samples annealed at 350, 400, 450 and 500℃ for 1 h were investigated. TEM observation indicated that tangled dislocation cells are typical microstructure in cold worked sample; After 350℃ annealing, the dislocations arrange regularly and the density decreases sharply, the alloy recovers partly and the grain size is about 500 nm; Further annealing to 500℃, recrystallization proceeds gradually in a wide temperature range due to the Zener drag effect of Al3(Sc, Zr) phase . As a result, the mechanical property changes greatly at 350℃ but keeps steady with further temperature increasing.
|
|
Received: 30 June 2005
|
|
|
[1] Willey L A. U S Pat 3619181, 1971 [2] Pan Q L, Yin Z M, Zhang C F. J Aeronaut Mater, 2002; 22:6 (潘青林,尹志民.张传福.航空材料学报, 2002;22:6) [3] Li H Z, Zhang Y H, Yin Z M, Pan Q L, Peng Z H. Rare Met Mater Eng, 1999; 28(2): 110 (李慧中,张永红,尹志民,潘青林,彭志辉.稀有金属材料与 工程,1999;28(2):110) [4] Bai Z H, Luo B H, Tai K P, Fan Y Q, Zhou H. Light Alloy Fabr Technol, 2004; 32(5): 48 (柏振海,罗兵辉,邰凯平,范云强,周华.轻合金加工技术, 2004;32(5):48) [5] Zhang L H, Liu J A. Light Alloy Fabr Technol, 2003; 31(10): 43 (张林和,刘静安.轻合金加工技术,2003;31(10):43) [6] Miura Y, Shioyama T, Kara D. Mater Sci Forum, 1996;217-222: 505 [7] Dougherty L M, Robertson I M, Vetrano J S. Acta Mater,2003; 51: 4367 [8] Riddle Y W, Sanders T H. Metall Mater Trans, 2004;35A: 341 [9] Doherty R D, Hughes D A, Humphreys F J, Jonas J J,Juul Jensen D, Kassner M E, King W E, McNelley T R,McQueen H J, Rollett A D. Mater Sci Eng, 1997; A238:219: |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|