| Micro-mechanisms of fatigue damage in copper crystals |
| ZHANG Zhefeng; DUAN Qiqiang; WANG Zhongguang |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences |
|
Cite this article:
ZHANG Zhefeng; DUAN Qiqiang; WANG Zhongguang. Micro-mechanisms of fatigue damage in copper crystals. Acta Metall Sin, 2005, 41(11): 1143-1149 .
|
|
|
Abstract Micro--mechanisms of fatigue damage in copper single-, bi- and poly- crystals were summarized in the present paper. A number of investigations reveal that fatigue crack
mainly initiates along persistent slip bands (PSBs) in copper single crystals at low or medium strain range, however, nucleates along coarse deformation bands (DBs) at high strain range. For copper bi-crystals, various large-angle grain boundaries (GBs) are always the preferential sites for the nucleation and propagation of fatigue
cracks while the low-angle GBs do not lead to fatigue cracking during fatigue. Fatigue
cracks mainly nucleated along large--angle GBs, sometimes along PSBs in polycrystalline copper, however, the initiation of fatigue crack at twin boundaries (TBs) was not observed due to the compatible slip deformation
across the TBs.
|
|
Received: 30 June 2005
|
|
|
[1] Forsyth P J E. Nature, 1953; 171: 172 [2] Thompson N, Wadsworth N J, Louat N. Philos Mag, 1956; 1: 113 [3] Kemsley D S, Paterson M S. Acta Metall, 1960; 8: 453 [4] Basinski S J, Basinski Z B, Howie A. Philos Mag, 1969; 19: 899 [5] Hancock J R, Grosskreutz J C. Acta Metall, 1969; 17: 77 [6] Mughrabi H. Mater Sci Eng, 1978; 33: 207 [7] Winter A T. Philos Mag, 1974; A30: 719 [8] Finney J M, Laird C. Philos Mag, 1975; A31: 339 [9] Mughrabi H, Ackermann F, Herz K. ASTM STP 811, 1983 [10] Kim W H, Laird C. Acta Metall, 1978; 26: 789 [11] Suresh S. Fatigue of Materials. 2nd ed, Cambridge Press, 1998: 27 [12] Cheng A S, Laird C. Mater Sci Eng, 1981; 51: 111 [13] Essmann U, Gosele U, Mughrabi H. Philos Mag, 1981; A44: 405 [14] Zhang Z F, Wang Z G, Sun Z M. Acta Mater, 2001; 49: 2875 [15] Li X W, Wang Z G, Li S X. Philos Mag, 2000; A80: 1901 [16] Li S X, Li X W, Zhang Z F, Wang Z G. Philos Mag, 2002; A82: 867 [17] Hu Y M, Wang Z G. Acta Mater, 1997; 45: 2655 [18] Hu Y M, Wang Z G. Scr Mater, 1996; 35: 1019 [19] Hu Y M, Wang Z G. Int J Fatigue, 1997; 19: 59 [20] Hu Y M, Wang Z G. Int J Fatigue, 1998; 20: 463 [21] Zhang Z F, Wang Z G, Li S X. Fatigue Fract Eng Mater Struct, 1998; 21: 1307 [22] Zhang Z F, Wang Z G, Hu Y M. Mater Sci Eng, 1999; A269: 136 [23] Zhang Z F, Wang Z G. Philos Mag, 1999; A79: 741 [24] Wang Z G, Zhang Z F, Li X W, Jia W P, Li S X. Mater Sci Eng, 2001; A319-321: 63 [25] Zhang Z F, Wang Z G. Z Metallkd, 2002; 93: 1188 [26] Hu Y M, Wang Z G, Li G Y. Mater Sci Eng, 1996; 208: 260 [27] Zhang Z F, Wang Z G. Acta Mater, 2003; 51: 347 [28] Zhang Z F, Wang Z G, Hu Y M. Mater Sci Eng, 1999; A272: 412 [29] Zhang Z F, Wang Z G. Philos Mag Lett, 2000; 80: 483 [30] Lim L C, Tay Y K, Fong H S. Acta Metall Mater, 1990; 38: 595 [31] Christ H J. Mater Sci Eng, 1989; A117: L25 [32] Liang F L, Laird C. Mater Sci Eng, 1989; A117: 103 [33] Heinz A, Neumann P. Acta Metall Mater, 1990; 38: 1933 [34] Ma B T, Laird C. Acta Metall, 1989; 37: 337 [35] Basinski Z B, Basinski S J. Prog Mater Sci, 1992; 36: 89 |