Abstract Doppler--broadening spectra of positron annihilation radiation of Al, Ti, V, Cr,
Mn, Fe, Co, Ni, Cu, Zn and Ga have been measured by using 2--detector coincidence technique.
The lower background of the spectrum allows to obtain the contribution of
annihilations with core electrons. The experiments
show that the background decreases with increasing the distance between the
sample and the Ge detector. The magnitude of the peak of the ratio curve of Ni
(ratio to Al) increases with decreasing the background of the spectrum. For Ti, V,
Cr, Mn, Fe, Co, Ni and Cu, the heights of the peaks in the ratio curves rise
with increasing the number of 3d--electrons.
|
Received: 01 March 2004
|
|
[1] West R N. Adv Phys, 1973; 22: 263 [2] Deng W, Xiong L Y, Wang S H, Guo J T, Long Q WActa Metall Sin, 2002; 38: 453(邓文,熊良钺,王淑荷,郭建亭,龙期威.金属学报,2002;38:453) [3] Lynn K G, MacDonald J R, Boie R A, Feldman L C,Gabbe J D, Robbins M F, Bonderup E, Golovchenko JPhys Rev Lett, 1977; 38: 241 [4] Deng W, Brusa R S, Karwarsz G P, Zec.ca A. Mater SciForum, 2001; 363: 195 [5] Deng W, Brusa R S, Karwarsz G P, Zecca A. Mater SciForum, 2001; 363: 198 [6] Saarinen K, Nissila J, Kauppinen H, Hakala M, Puska MJ, Hautojavi P, Corbel C. Phys Rev Lett, 1999; 82 1883 [7] Petkov M P, Weber M H, Lynn K G, Crandall R S, GhoshV J. Phys Rev Lett, 1999; 82. 3819 [8] Ghosh V J, Alatalo M, Asoka-Kumar P, Nielsen B, LynnK G. Phys Rev, 2000; 61B: 10092 [9] Mylar U, Simpson P J. Phys Rev B, 1997; 56: 14303 [10] Asoka-Kumar P, Alatalo M, Ghosh V J. Kruseman A C,Noelsen B, Lynn K G. Phys Rev Lett, 1996; 82: 2097 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|