Abstract The experiment of a coupling effect
on propagation of unloaded indentation cracks in a PZT--5H ceramic
shows that residual
stress itself is too small to induce delayed propagation
of the indentation crack in silicon oil. If
applied constant electric field is larger than
0.2 kV/cm, the coupling of electric field, residual stress
and silicon oil can cause delayed propagation of the
crack after incubation time, but the crack will arrest after
propagating for 10---30 um because of decrease of the stress
intensity factor with increasing the crack length. The threshold
electric field of delayed propagation of the
crack in silicon oil is EDP=0.2 kV/cm. If the
field is larger than the critical field of 5.25 kV/cm,
coupling of the electric field and residual stress is enough to cause
instant propagation of the crack
and propagates continuously, then arrests if under the constant
electric field. If the applied field is
larger than 12.6 kV/cm, even if no residual
stress, the electric field itself can make many
cracks initiate, grow and connect in a smooth specimen,
resulting in delayed failure. The threshold
electric field of delayed failure of a smooth
specimen in silicon oil is 12.6 kV/cm and the
critical electric field for instant failure is EF=19.1
kV/cm.
|
|
Received: 01 March 2004
|
|
|
[1] Yang W. Mechatronic Reliability. Beijing: Tsinghua Uni-versity Press, 2001; 151(杨卫.力电失效学.北京:清华大学出版社,2001:151) [2] Tobin A G, Pak Y E. Proc SPIE Int Soc Opt Eng, 1993;1916: 78 [3] Wang H Y, Singh R N. J Appl Phys, 1997; 81: 7471 [4] Sun C T, Park S. Proc SPIE Int Soc Opt Eng, 1995; 2441:213 [5] Chantikul P, Anstis G R, Laun B R, Marshall D B. J AmCeram Soc, 1981; 64: 539 [6] Wang Y, Chu W Y, Su Y J, Qiao L. Mater Lett, 2003; 57:1156 [7] Wang Y, Chu W Y, Su Y J. Mater Sci Eng, 2002; 95B:263 [8] Wang Y, Chu W Y, Su Y J, Gao K W, Liu H, Qiao L J.Acta Metall Sin, 2002; 39: 182(王毅,褚武扬,宿彦京,高克玮,刘辉,乔利杰.金属学报,2002;39:182) [9] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. ApplPhys Lett, 2003; 82: 1583 [10] Michalske T A, Freiman S W. J Am Ceram Soc, 1983; 66:284 [11] Freiman S W, White G S, Fuller J R. J Am Ceram Soc,1985; 68: 108 [12] Huang H Y, Chu W Y, Su Y J, Gao K W, Qiao L J. ActaMetall Sin, 2004; 41: 962(黄海友,褚武扬,宿彦京,高克玮,乔利杰.金属学报,2004;41:962) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|