Acta Metall Sin  1998, Vol. 34 Issue (9): 903-907    DOI:
Current Issue | Archive | Adv Search |
STICKING FAULT ENERGY CALCULATING OF TWO KINDS OF STAINLESS IRON BASED SHAPE MEMORY ALLOYS
LIU Xiangjun; LIN Xinyuan; CHEN Shiren (Institute for Materials Research; Fuzhou University; Fuzhou 350002)Correspondent: CHEN Shiren; professor Tel: (0591)3728486; Fax. (0591)3713866;E-mail: material@fzu. edu.cn
Cite this article: 

LIU Xiangjun; LIN Xinyuan; CHEN Shiren (Institute for Materials Research; Fuzhou University; Fuzhou 350002)Correspondent: CHEN Shiren; professor Tel: (0591)3728486; Fax. (0591)3713866;E-mail: material@fzu. edu.cn. STICKING FAULT ENERGY CALCULATING OF TWO KINDS OF STAINLESS IRON BASED SHAPE MEMORY ALLOYS. Acta Metall Sin, 1998, 34(9): 903-907.

Download:  PDF(903KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Stacking fault energies in Fe-Mn-Si-Cr-Ni and Fe-Mn-Si-Cr-Ni-Co stainless iron-based shape memory alloys are calculated by means of extended dislocation node measurement,and the corresponding values are 25.1 and 10.3×10-7 J/cm2 respectively.
Key words:  iron-based shape memory alloy      dislocation node      stacking fault energy      Fe-Mn-Si-Cr-Ni system      Fe-Mn-Si-Cr-Ni-Co system     
Received:  18 September 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I9/903

1 Fujita H,Ueda S.ActaMetall,1972;20:759
2 Welan J A. Proc Roy Soc, 1958; A249
3 Hirsch P, Howie A, Nicholson R B, Pashley D W, Whelan M J. ELectronMicroscopy of Thin Crystals, New York, Roberte Krieger Publishing Company, 1977: 430
4 Brown L M. Philos Mag, 1965; 12: 191
5 Jian Li,Wayman C M, Scr Metall Mater, 1992; 27: 279
6 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897
[1] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[2] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[3] YANG Zhikun, WANG Hao, ZHANG Yiwen, HU Benfu. Effect of Ta Content on High Temperature Creep Deformation Behaviors and Properties of PM Nickel Base Superalloys[J]. 金属学报, 2021, 57(8): 1027-1038.
[4] Zongwei JI,Song LU,Hui YU,Qingmiao HU,Levente Vitos,Rui YANG. First-Principles Study on the Impact of Antisite Defects on the Mechanical Properties of TiAl-Based Alloys[J]. 金属学报, 2019, 55(5): 673-682.
[5] AN Xianghai, WU Shiding, ZHANG Zhefeng. INFLUNECE OF STACKING FAULT ENERGY ON THE MICROSTRUCTURES, TENSILE AND FATIGUE PROPERTIES OF NANOSTRUCTURED Cu-Al ALLOYS[J]. 金属学报, 2014, 50(2): 191-201.
[6] XUE Peng, XIAO Bolü, MA Zongyi. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR PROCESSED ULTRAFINE-GRAINED AND NANOSTRUCTURED Cu-Al ALLOYS[J]. 金属学报, 2014, 50(2): 245-251.
[7] QIN Xiaomei CHEN Liqing DI Hongshuang DENG Wei. EFFECT OF DEFORMATION TEMPERATURE ON TENSILE DEFORMATION MECHANISM OF Fe-23Mn-2Al-0.2C TWIP STEEL[J]. 金属学报, 2011, 47(9): 1117-1122.
[8] DONG Minghui HAN Peide ZHANG Caili YANG Yanqing ZHANG Lili LI Hongfei. FIRST-PRINCIPLES STUDY OF STACKING FAULT ENERGY AND DEFORMATION TWIN\par ENERGY IN Al-Mg ALLOYS[J]. 金属学报, 2011, 47(5): 573-577.
[9] WANG Shuhan LIU Zhenyu ZHANG Weina WANG Guodong. INVESTIGATIONS ON TEMPERATURE DEPENDENCE OF MECHANICAL PROPERTIES AND THE DEFORMATION MECHANISM OF A TWIP STEEL[J]. 金属学报, 2009, 45(5): 573-578.
No Suggested Reading articles found!