Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (9): 897-902    DOI:
Current Issue | Archive | Adv Search |
STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM
LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn
Cite this article: 

LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn. STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM. Acta Metall Sin, 1998, 34(9): 897-902.

Download:  PDF(1174KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A simple type of diffusion couple was designed. The compositions of the phase equilibrium α/γ at 1200℃ and 1250℃ in Ti-Al-Cr-Fe quarternary system have been determined by the diffusion couple-electron probe method, and partial isothermal squares for Ti-Al-Cr-Fe quarternary system have been drawn. The results show that Cr has the effect of increasing the solubility for Fe in the α phase and Fe has the effect of increasing the solubility for Cr in the α phase.
Key words:  Ti-Al-Cr-Fe quarternary system      phase equilibrium     
Received:  18 September 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I9/897

1 Kim Y W .JOM, 19895 41(7):24
2 Kim Y W JOM,1994;46(7):30
3 山口正治,乾晴行,日井泰治金属,1995;65:215(Yamaguchi M, Inui H; Shiroi T, Met Technol, 1995; 65: 215)
4 桥本健纪,土肥春夫,还本得藏,铃木朝夫日本金属学会志,1988;52(8):816(Hashimoto K,Doi H,Kasahara K;Tsujimoto T,SuzukiT.J Jpn Inst Met,19882 52:816)
5 Nakagawa Y G, Yokoshima S, Matsuda K. Mate, Sci Eng, 1992; A153: 722
6 丁进军,赵刚,郝士明金属学报,19972 33:1105(Ding J J, Zhao G, Hao S M. Acta Metall Sinica, 1997 33: 1105)
7 李俊涛,郝士明东北大学学报,1997;18:362(Li J T, Hao S M. J Northeastern University, 1997 18: 362)
8 蒋敏,郝士明中国物理协会第六届全国相图学术会议论文集,1990:150(Jiang M,HaoS M.Proceedings of the 6th NationalSymposium on Phase Diagrams, Commission on Phase Diagrams of the Chinese Physical Societyl1990:150)
9 丁进军,赵刚,蒋敏,郝士明材料研究学报, 1998(in Press)(Ding J J, Zhao G, Jian M. Chin J Mat Res, 1998(in press))A
[1] LI Hongxiao REN Yuping MA Qianqian JIANG Min QIN Gaowu. PHASE EQUILIBRIUM IN THE LOW-Ca SIDE OF Mg-Zn-Ca SYSTEM AT 400 ℃[J]. 金属学报, 2012, 48(1): 70-75.
[2] LI Hongxiao MA Qianqian REN Yuping JIANG Min QIN Gaowu. TERNARY COMPOUNDS AND RELATIVE PHASE EQUILIBRIA IN THE Mg-RICH SIDE OF THE Mg-Zn-Ca SYSTEM[J]. 金属学报, 2011, 47(4): 385-390.
[3] XIE Yu ZHANG Yan CHEN Rongshi HAN Enhou. RELATIONSHIP OF COMPOSITIONS, PHASE CONSTITUENTS AND SOLIDIFICATION PATHS OF CASTING Mg-Al-Zn ALLOYS[J]. 金属学报, 2009, 45(11): 1396-1401.
[4] ;. Research on the ternary compound T1 with low Nd content in the Mg-Zn-Nd alloys[J]. 金属学报, 2008, 44(4): 385-390 .
[5] FU Xiaoliang; LI Changrong; LI Mei; ZHANG Weijing. Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃[J]. 金属学报, 2005, 41(7): 691-694 .
[6] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[7] LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006). ^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM[J]. 金属学报, 1996, 32(11): 1171-1176.
[8] QIN Gaowu;HAO Shiming;ZENG Ninghua (Northeastern University;Shenyang 110006)(Manuscript received 1994-11-04;in revised form 1995-05-04). α(α_2)/γ PHASE EQUILIBRIA IN Ti-Al-Ga AND Ti-Al-Nb-Cr SYSTEMS[J]. 金属学报, 1995, 31(23): 484-488.
[9] LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang). ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM[J]. 金属学报, 1992, 28(7): 50-54.
[10] HAO Shiming; JIANG Min (Northeast University of Technology; Shenyang). TWO-PHASE EQUILIBRIUM CALCULATION BY THE GRAND POTENTIAL METHOD FOR BINARY ALLOYS[J]. 金属学报, 1992, 28(11): 54-58.
No Suggested Reading articles found!