| MICROYIELD BEHAVIOURS OF SiCp/2024A1 COMPOSITE AND 2024A1 ALLOY |
| ZHANG Fan; LI Xiaocui; JIN Cheng; QIU Jiming; HU Zhengjun(The State Key Laboratory of Metal Matrix Composites; Shanghai Jiaotong University; Shanghai 200030) |
|
Cite this article:
ZHANG Fan; LI Xiaocui; JIN Cheng; QIU Jiming; HU Zhengjun(The State Key Laboratory of Metal Matrix Composites; Shanghai Jiaotong University; Shanghai 200030). MICROYIELD BEHAVIOURS OF SiCp/2024A1 COMPOSITE AND 2024A1 ALLOY. Acta Metall Sin, 1998, 34(7): 713-718.
|
|
|
Abstract microyield behaviours of SiCp/2024A1 composite and its matrix alloy were investigated in this work. The results indicated that the composite showed quite different strain relaxation before" general" microyielding and its microyield mechanism was not same as that of the matrix alloy. It was also showed that during aging treatment, the microyield strengths of both composite and matrix alloy were dependent to precipitation of the strengthening phase,S', and exhibited a peak aging trend. Thermal cycling treatment could improve the microyield strength of the matrix alloy, but lower the microyield strength of the composite.
|
|
Received: 18 July 1998
|
1 Mohn W R, Vukoratovic D. SAMPE J, 1988; (1/2): 1 2 Hamann R, Gobin P F, Fougeres R. Scr Metall Mater 1990; 24: 1789 3李志林,姚忠凯兵器材料科学与工程,1991;(11):1(Li Zhilin, Yao Zhongkai. Ordance Mate, Sci Eng, 1991(11):1) 4李义春,安希镛、中国有色金属学报,1992;2(3):76(Li Yichun; An Xiyong.Chin J Nonferrous Met, 1992; 2(3): 76) 5 Croucher T, Butler D. Heat Treat,1980;(9): 24 6 Hunsicker H Y. Metall Trans, 1980; 11A: 759 7张帆,李小璀,钟锋,金城 热加工工艺,1997;(3):31 (Zhang Fan,Li Xiaocui,Zhong Feng,Jin Cheng.Hot Work Technol,1997(3):31) 8 Carnahan R D, Arsenault R J, Stone G A. Trans Metall Soc AIME, 1967; 239: 1193 9 Arsenault R J. Mater Sci Eng, 1984; 64: 171 10 Vogelsang M, Arsenault R J, Fisher R M. Metall Trans, 1986; 17A: 379 11 Arsenault R J, Shi N. Mater Sci Eng, 1986; 81: 175 12 Brown N, Lukens K F. Acta Metall, 1961; 9: 106 13 Marchall C V, Maringer R E. Dimensional Instabitity. New York: Pergamon Press, 1977: 139d |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|