EFFECT OF Ni_xAl_yTi_z REFINER ON GRAIN STRUCTURES OF CAST SUPERALLOY K4169
ZHENG Jianbang; DING Hao; GUO Yiping; LIU Lin (Department of Applied Physics; Northwestern Polytechnical University; Xi'an 710072)LIU Wei; LI Xingjian (Liming Engine Manufacturing Company; Shenyang 110043)
Cite this article: 

ZHENG Jianbang; DING Hao; GUO Yiping; LIU Lin (Department of Applied Physics; Northwestern Polytechnical University; Xi'an 710072)LIU Wei; LI Xingjian (Liming Engine Manufacturing Company; Shenyang 110043). EFFECT OF Ni_xAl_yTi_z REFINER ON GRAIN STRUCTURES OF CAST SUPERALLOY K4169. Acta Metall Sin, 1998, 34(4): 362-366.

Download:  PDF(2758KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Grain size and dendrite morphologies of Fe-Ni based superalloy K4169 were investigated with the melt addition of NixAlyTiz refiner. It is found that the grain size of ingotscan be refined obviously to 0.1-0.2mm, close to the order of ASTM 1-3, by lowering the melting homogeneous treatment temperature during the melting and casting process. In addition, the microstructure of grains can be transferred from dendritic to cellular due to the addition ofrefiner at the same cooling condition. The addition of NixAlyTiz refiner has the advantages of little influence on the freezing characters, alloy composition as well as phase constitution.
Key words:  Fe-Ni superalloy      grain refinement      nucleant      dendrite morphology     
Received:  18 April 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I4/362

1 Woulds M, Benson H. In: Gell M, Kortovich C S, Bricknell R H, Kent W B, Radavich J F eds., Superalloys,Champion: The Metallurgical Society of AIME, 1984: 3
2 Ewing B A, Green K A. In: Gell M, Kortovich C S, Bricknell R H, Kent W B, Radavich J F eds., Superalloys,Champion: The Metallurgical Society of AIME, 1984: 33
3 Mclean M. Mater Sci Technol, 1988; 4: 205
4 Prichard P D, Dalal R P. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D,Klarstrom D L eds., Superalloys. Champion: The Metallurgical Society of AIME, 1992: 205
5 Nazmy M, Weiss B, Sticbler R. High Temperature Materials for Power Engineering II Liege: Kluwer Academic PubIishers, 1990: 1397
6 赵惠田, 师昌绪. 金属学报, 1981; 17: 118(Zhao Huitian, Shi Changxu. Acta Metall Sin, 1981; 17: 118)
7 Tien J K, Borofka J C, Casey M E. J Met, l986; 38: 13
8 刘林. 航空学报. 1994; 15: 1357 (Liu Lin. Acta Aeronaut Astronaut Sin, 1994; 15: 1357)
9 Liu L, Zhen B L, Banerji A, Reif W, Sommer F. Scr Metall Maten 1994; 30: 593
10 Bramfitt B L. Metall Trans, 1970; 1: 1987`
[1] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[2] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
[3] LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie. Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. 金属学报, 2022, 58(3): 365-374.
[4] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[5] LI Xiucheng,SUN Mingyu,ZHAO Jingxiao,WANG Xuelin,SHANG Chengjia. Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels[J]. 金属学报, 2020, 56(4): 653-660.
[6] WU Huajian, CHENG Renshan, LI Jingren, XIE Dongsheng, SONG Kai, PAN Hucheng, QIN Gaowu. Effect of Al Content on Microstructure and Mechanical Properties of Mg-Sn-Ca Alloy[J]. 金属学报, 2020, 56(10): 1423-1432.
[7] ZHANG Jun,JIE Ziqi,HUANG Taiwen,YANG Wenchao,LIU Lin,FU Hengzhi. Research and Development of Equiaxed Grain Solidification and Forming Technology for Nickel-Based Cast Superalloys[J]. 金属学报, 2019, 55(9): 1145-1159.
[8] Liping DENG,Kaixuan CUI,Bingshu WANG,Hongliang XIANG,Qiang LI. Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. 金属学报, 2019, 55(8): 976-986.
[9] Shubo LI, Wenbo DU, Xudong WANG, Ke LIU, Zhaohui WANG. Effect of Zr Addition on the Grain Refinement Mechanism of Mg-Gd-Er Alloys[J]. 金属学报, 2018, 54(6): 911-917.
[10] Yizhe MAO, Jianguo LI, Lei FENG. Effect of Coarse β(Al3Mg2) Phase on Microstructure Evolution in 573 K Annealed Al-10Mg Alloy by Uniaxial Compression[J]. 金属学报, 2018, 54(10): 1451-1460.
[11] Lili ZHANG, Hongxiang JIANG, Jiuzhou ZHAO, Lu LI, Qian SUN. A New Understanding Toward Effect of Solute Ti on Grain Refinement of Aluminum by Al-Ti-B Master Alloy: Kinetic Behaviors of TiB2 Particles and Effect of Solute Ti[J]. 金属学报, 2017, 53(9): 1091-1100.
[12] Zhiqiang ZHANG,Limin DONG,Shaoxuan GUAN,Rui YANG. Microstructure and Mechanical Properties of TC16 Titanium Alloy by Room Temperature Roller Die Drawing[J]. 金属学报, 2017, 53(4): 415-422.
[13] Ning LI,Rong ZHANG,Limin ZHANG,Hui XING,Pengfei YIN,Yaoyan WU. Study on Grain Refinement Mechanism of Hypoeutectic Al-7%Si Alloy Under Low Voltage Alternating Current Pulse[J]. 金属学报, 2017, 53(2): 192-200.
[14] Jinrong ZUO,Longgang HOU,Jintao SHI,Hua CUI,Linzhong ZHUANG,Jishan ZHANG. PRECIPITATES AND THE EVOLUTION OF GRAIN STRUCTURES DURING DOUBLE-STEP ROLLING OF HIGH-STRENGTH ALUMINUM ALLOYAND RELATED PROPERTIES[J]. 金属学报, 2016, 52(9): 1105-1114.
[15] Yuefei TENG,Yingju LI,Xiaohui FENG,Yuansheng YANG. EFFECT OF RECTANGLE ASPECT RATIO ON GRAIN REFINEMENT OF SUPERALLOY K4169 UNDER PULSED MAGNETIC FIELD[J]. 金属学报, 2015, 51(7): 844-852.
No Suggested Reading articles found!