Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (3): 232-236    DOI:
Current Issue | Archive | Adv Search |
THE RELATIONSHIPS BETWEEN THE MARTENSITE VARIANTS IN Cu-BASED SHAPE MEMORY ALLOYS ANALYSED WITH PHENOMENOLOGICAL THEORV AND GROUP THEORY
ZHANG Jianxin; ZHENG Yeing; CAI Wei; ZHAO Liancheng(School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001)
Cite this article: 

ZHANG Jianxin; ZHENG Yeing; CAI Wei; ZHAO Liancheng(School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001). THE RELATIONSHIPS BETWEEN THE MARTENSITE VARIANTS IN Cu-BASED SHAPE MEMORY ALLOYS ANALYSED WITH PHENOMENOLOGICAL THEORV AND GROUP THEORY. Acta Metall Sin, 1998, 34(3): 232-236.

Download:  PDF(415KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The habit planes of martensite variants in Cu-based shape memory alloys are calculated with phenomenological crystallographic theory and the probable types of inter-variant boundaries are analysed with group theory. The results show that there are four kinds of twin relationships, i.e., reflection twin, 180°rotation twin, 120° rotation twin, and 90°rotation twin.
Key words:  Cu-based shape memory alloy      boundary      phenomenological theory      group theory      twin     
Received:  18 March 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I3/232

1 Adachi K, Perkins J, Wayman C M. Acta Metall, 1988; 36: 1343
2 Wayman C M. Intnduction to the Crystallography of Mariensitic Transformations.New York: The McMillan Co, 1964: 59
3 朱伟光, 江伯鸿, 徐祖耀. 金属学报, 1986; 22: A229(Zhu Weiguang, Jiang BOhong, Xu Zuyso. Acta Metall Sin, 1986; 22: A229)
4 Zhu Weiguang, Cheng Weiye, Xu Zuyao (T. Y. Hsu). Acta Metall, 1985; 33: 2075
5 Wang Baoqi, Gu Nanju, Yin Fuxing, Wang Ruisiang, Zhang Jianxin.Trans Mater Res Soc Jpn, 1994; 18B:947
6 Chakravorty S, Wayman C M. Acta Metall, 1977; 25: 989
7 Zhu M, Yang D Z, Kuo K X. Acta Metall, 1988; 36: 1329
8 Portier R, Gratias D. i Phys Colloq, 1982; C4(Suppl.): 17
9 Guymont M, Gratias D, Portier R, Fayard M. Phys Status Solidi, 1976; A38: 629
10王仁卉,郭可信晶体学中的对称群.北京:科学出版社,1990(Wang Renhui, Guo Kexin. Sytnmetry GrotLP in CrystallWhy. Beijing: Science Press, 1990)11 Guymont M. Phys Rev, 1978; B18: 5385
12朱伟光,陈伟业,徐祖耀、金属学报,1986;22:A236(Zhu Weiguang, Chen Weiye, Xu Zuyao. Acta Metall Sin, 1986; 22: A236)
13 Adachi K, Perkins J, Wayman C M. Acta Metall, 1986; 34: 2471
14 Saburi T, Nenno S. In: Aaronson H I, Wayman C M eds., Proc Int Conf on Solid to Solid Transformations,New York: B utterworth-Heinemann Ltd, 1982: 1455
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[3] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[4] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[5] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[6] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[7] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[8] XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui. Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing[J]. 金属学报, 2023, 59(5): 693-702.
[9] SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang. Unravelling the {101¯2} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy[J]. 金属学报, 2023, 59(4): 556-566.
[10] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
[11] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[12] LI Xin, JIANG He, YAO Zhihao, DONG Jianxin. Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr[J]. 金属学报, 2023, 59(2): 309-318.
[13] YANG Du, BAI Qin, HU Yue, ZHANG Yong, LI Zhijun, JIANG Li, XIA Shuang, ZHOU Bangxin. Fractal Analysis of the Effect of Grain Boundary Character on Te-Induced Brittle Cracking in GH3535 Alloy[J]. 金属学报, 2023, 59(2): 248-256.
[14] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[15] GAO Dong, ZHOU Yu, YU Ze, SANG Baoguang. Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature[J]. 金属学报, 2022, 58(9): 1141-1149.
No Suggested Reading articles found!