| CYCLIC DEFORMATION BEHMIOR AND FATIGUE CRACK INITIATION IN COPPER BICRVSTALS |
| HU Yunming;WANG Zhongguang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)Correspondent; HU Yunming; Tel: (024)23843531-55gg5; Fax: (024)23891s20Manuscript received 1997-12-17; in revised form 1998-01-30 |
|
Cite this article:
HU Yunming;WANG Zhongguang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)Correspondent; HU Yunming; Tel: (024)23843531-55gg5; Fax: (024)23891s20Manuscript received 1997-12-17; in revised form 1998-01-30. CYCLIC DEFORMATION BEHMIOR AND FATIGUE CRACK INITIATION IN COPPER BICRVSTALS. Acta Metall Sin, 1998, 34(12): 1255-1260.
|
|
|
Abstract The fatigue cracking behavior and mechanisms in three types of [34] iso-axialcopper bicrystals have been studied by using scanning electron microscopy (SEM). One bicrystalcontains a grain boundary (GB) perpendicular to the loading direction and the two others containtilting GBs. The experimental results show that the intergranular fatigue cracking is the mainmode in the fatigue failure for the three types of copper bicrystals. However, the fatigue craCkingmechanisms are different for the perpendicular GB bicrystal and the tilting GB bicrystals. Theintergranular fatigue cracks are mainly formed by impingement of persistent slip bands againstthe GB in the perpendicular GB bicrystal. While the fatigue cracking initiation is predominatelydetermined by the stress concentration resulted from steps for the tilting GB bicrystal. The foregoing difference between the fatigue cracking initiation mechanisms in the two types of bicrystalsis closely related to the specimens geometry with respect to the primary slip systems.
|
|
|
1 Kim W H, Laird C Acta Metall, 1978; 26: 777 2 Kim W H, Laird C Acta Metall, 1978; 26: 789 3 Lim L C. Acta Metal 1986; 35: 1653 4Figueroa J C,Laird C.Mater Sci Eng,1983;60:45 5 Llanes L, Laird C. Mater Sci Eng, 1992; 57A: 21 6 Katsgirik K, Omura A, Koyanagik, Awatani J, Shiraishi T, Kaneshiro. Metall Trans , 1977; SA: 1769 7 Mughrabi H; Wang R, Differt K, Essmann U. ASTM STP 811, 1983: 5 8 Liu W,Bayerlein M ,Mughrabi H,Day A,Quested P N Acta Metall Mater,1992;40:1963 9 Christ H J Mate, Sci Eng, 1989 All7: L25 10刘蔚中国科学院金属研究所硕士学位论文,1987 (Liu w.Master Disertation Institute of Metal Reserch,The Chinese Academy of Sciences,1987) 11胡运明,王中光金属学报,19972 33:824 (Hu Y M, Wang Z G Acta Metall Sin, 1997; 33: 824) 12胡运明,王中光.金属学报,1997;33:814 (Hu Y M, Wang Z G. Acta Metall Sin.1997; 33: 814)O |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|