Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (12): 1261-1266    DOI:
Current Issue | Archive | Adv Search |
DIRECTIONAL COARSENING OF THE γ'-PHASE DURING COMPRESSION CREEP OF A SINGLE CRVSTAL NICKEL-BASE SUPERALLOY
(TIAN Sugui ; ZHOU Huihua; ZHANG Jinghua;YANG Hongcai;XU YOngboHU Zhuangqi(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal ReSearch; The Chinese Academyof Sciences; Shenyang 110015)(Department of Materials Sciences and Engineering; Northeastern University; Shenyang 110006)(Department of Metal Materials Engineering; Shenyang Polytechnic University 110023)Correspondent:TIAN Sugui; associate professor; Tel: (o24)-25927399; Fax: (024)e3891s2oManuscript received 1997-12-23; in revised form 1998-03-16
Cite this article: 

(TIAN Sugui ; ZHOU Huihua; ZHANG Jinghua;YANG Hongcai;XU YOngboHU Zhuangqi(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal ReSearch; The Chinese Academyof Sciences; Shenyang 110015)(Department of Materials Sciences and Engineering; Northeastern University; Shenyang 110006)(Department of Metal Materials Engineering; Shenyang Polytechnic University 110023)Correspondent:TIAN Sugui; associate professor; Tel: (o24)-25927399; Fax: (024)e3891s2oManuscript received 1997-12-23; in revised form 1998-03-16. DIRECTIONAL COARSENING OF THE γ'-PHASE DURING COMPRESSION CREEP OF A SINGLE CRVSTAL NICKEL-BASE SUPERALLOY. Acta Metall Sin, 1998, 34(12): 1261-1266.

Download:  PDF(2387KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructures of a single crystal nickel-base superalloy with [001] orientation at different creep stages of the constant loading compression were observed by meansof TEM and SEM. The results showed that the strip--like rafts were formed along the directionparallel to the stress axis in a mode of the side plane link in primary creep. The applied stressresulted in the decrease of coherent strain and energy of the 7i/7 interfaces parallel to the stressaxis The energy released was supposed to be the driving force for the diffusion elements. Bycompared compressive creep with tensile, the longer time and bigger stress were needed for ther' rafted.
Key words:  single crystal nickel-base superalloy      compression creep      directional coarsening      driving force     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I12/1261

1Tien J K; Copley S M. Metall Trans, 1971; 2: 215
2Pollock T M, Argon A S. Acta Metall Mater, 1994; 42: 1859
3Muller L, Glatzel U; Feller—Kniepmeier M. Acto Metall Mater, 1992 40: 121
4彭志方, Glatzel U, Feller—Kniepmeier M.金属学报,1995; 31(12): A531(Peng z F,Glatzel U,Feller-Kniepmeier M.Acta Metall Sin ,995; 31: A531)
5田素贵,周惠华,张静华,杨洪才,徐永波,胡壮麒.金属学报,1998:34(6):A591(Tian S G, Zhou H H, Zhang J H, Yang H C, Xu Y B, Hu Z Q. Acta Metall Sin ,1998 34(6): A591)
6秦高梧,郝士明.金属学报,1995;31(11):B485(Qin G W, Hao S M. Acta Metall Sin, 1995; 31: B485)
7Pollock T M,Argon A S.Acta Metall Mater,1992;40(1):1M
[1] WANG Bin, LIU Zhenyu, ZHOU Xiaoguang, WANG Guodong. CALCULATION OF TRANSFORMATION DRIVING FORCE FOR THE PRECIPITATION OF NANO-SCALED CEMENTITES IN THE HYPOEUTECTOID STEELS THROUGH ULTRA FAST COOLING[J]. 金属学报, 2013, 49(1): 26-34.
[2] Na Wang; Zhenmin Du. Driving Force for the Nucleation from Supercooled Liquid and Thermodynamic Analysis of Glass Forming Ability for Binary Alloys[J]. 金属学报, 2008, 44(9): 1111-1115 .
[3] XingFu Yu. Microstructure Evolution of A Pre-compression Nickel-Base Single Crystal Superalloys During Tensile Creep[J]. 金属学报, 2008, 44(8): 961-967 .
[4] XIONG Ying. A TWO-PARAMETER DRIVING FORCE FOR FATIGUE CRACK GROWTH[J]. 金属学报, 2008, 44(11): 1348-1353 .
[5] 许良红 Xu Liang-Hong; tian zhiling Tian. The investigation of the oriented precipitate-free zone in high strength aluminum alloy welds[J]. 金属学报, 2008, 44(1): 91-97 .
[6] TIAN Sugui ; ZHOU Huihua ; ZHANG Jinghua; YANG Hongcai ; XU Yongbo;HU Zhuangqi ( State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)( Department of Materials Science and Engineering; Northeastern University ; Shenyang 110006)( Department of Materials Science and Engineering; Shenyang Polytechnic University; Shenyang 110023)Correspondent: TIAN Sugui; associate professor Tel: (024)5927399. A DIRECTIONAL COARSENING MECHANISM OF THE γ'-PHASE DURING CREEP OF A SINGLE CRYSTAL NICKEL-BASE SUPERALLOY[J]. 金属学报, 1998, 34(6): 591-596.
[7] TIAN Sugui;ZHOU Huihua;ZHANG Jinghua;YANG Hongcai;XU Yongbo;HU Zhuangqi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)(Department of Metal Materials and Engineering; Shenyang Polytechnic University; Shenyang 110023). DISLOCATION CONFIGURATION IN SINGLE CRYSTAL NICKEL-BASE ALLOY DUING PRIMARY CREEP[J]. 金属学报, 1998, 34(2): 123-128.
[8] TIAN Sugui;ZHOU Huihua; ZHANG Jinghua; YANG Hongcai; XU Yongbo; HU Zhuangqi (State key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)(Department of Metal Materials Engineering; Shenyang Polytechnic University; Shenyang 110023). THE CREEP-DAMAGE BEHMIOUR OF A SINGLE CRYSTAL NICKEL-BASE SUPERALLOY[J]. 金属学报, 1998, 34(1): 57-62.
[9] YUE Zhufeng;LU Zhenzhou;ZHENG Changqing(Northwestern Polytechnical University;Xi'an 710072). THE CREEP─DAMAGE BEHAVIOUR FOR SINGLE CRYSTAL NICKEL-BASE SUPERALLOY[J]. 金属学报, 1995, 31(8): 370-375.
[10] PENG Zhifang (Wuhan University of Hydraulic and Electric Engineering; Wuhan 430072); GLATZEL Uwe; FELLER-KNIEPMEIER Monika(Technische Universitat Berlin; Germany). DIRECTIONAL COARSENING OF γ'PRECIPITATES IN A SINGLE CRYSTAL NICKEL BASE SUPERALLOY[J]. 金属学报, 1995, 31(12): 531-536.
[11] YANG Liu;LIU Shikai;YANG Ping Southwest Jiaotong University; Chengdu. CALCULATION OF BAINIT TRANSFORMATION KINETICS IN Fe-C-Si-Mn ALLOYS[J]. 金属学报, 1993, 29(1): 1-5.
[12] LIN Guangming;HUANG Yuanshi;ZHANG Jinxiu Zhongshan University; Guangzhou LIN Guangming; Associate Professor; Department of Physics; Zhongshan University;Guongzhou 510275. TRANSFORMATION OF TWO WAY SHAPE MEMORY MATERIAL CONSTRAINED BY STRESS[J]. 金属学报, 1989, 25(6): 16-21.
[13] XIE Changsheng;SUN Peizhen;CHEN Yuqiu;ZHAO Jiansheng Huazhong University of Science and Technology. QUASI-EQUILIBRIUM MICROSTRUCTURES AND EFFECT OF ALLOY ELEMENTS IN Fe-Mn-Ni-Cr STEELS[J]. 金属学报, 1989, 25(4): 54-59.
No Suggested Reading articles found!