Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (10): 1028-1032    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF QUENCHING CONDITIONS AND MICRO-ADDITION OF CERIUM ON THERMAL STABILITY OF AMORPHOUS Fe-B-Si ALLOYS
CHE Xiaozhou; ZHU Min; LI Zuxin(Department of Mechano-Electronic Engineering; South China University of Technology; Guangzhou 510641)DAI Lizhi(Central Iron and Steel Research Institute; Beijing 100081)Correspondent: CHE Xiaozhou;associate professor;Tel: (020)87111317
Cite this article: 

CHE Xiaozhou; ZHU Min; LI Zuxin(Department of Mechano-Electronic Engineering; South China University of Technology; Guangzhou 510641)DAI Lizhi(Central Iron and Steel Research Institute; Beijing 100081)Correspondent: CHE Xiaozhou;associate professor;Tel: (020)87111317. INFLUENCE OF QUENCHING CONDITIONS AND MICRO-ADDITION OF CERIUM ON THERMAL STABILITY OF AMORPHOUS Fe-B-Si ALLOYS. Acta Metall Sin, 1998, 34(10): 1028-1032.

Download:  PDF(508KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influences of melt spun parameters and dricro-addition of cerium on thermal stability of amorphous Fe-B-Si alloys have been studied. The higher cooling speed foras-quenched amorphous ribbon, the more difficult for structural relaxation in low-temperatureannealing process. Experimental results show no direct relationship between the quenching condition and crystallization for Fe80B11.5Si8.5 metallic glass. Optimal addition of cerium obviouslyretard the ductile-to-brittle transition process in structural relaxation stage, when annealingtemperature is low. At high temperature annealing stage, the addition of cerium lowers the onsettemperature of crystallization; and this effect is in direct proportion to the content of cerium inribbons.
Key words:  amorphous Fe-B-Si      thermal stability      quenching condition      rare-earth element     
Received:  18 October 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I10/1028

1车晓舟.金属学报, 1995; 31: B418(Che X Z. Acta Metall Sin, 1995; 31: B418)
2姚斌,华中,闵春宗,王爱民,刘浩哲,丁炳哲,胡壮麟.金属学报,1996;32:867(Yao B, Hua Z, Min C Z, Wang A M, Liu H Z, Ding B Z, Hu Z Q. Acta Metall Sin, 1996; 32: 867)
3沈德久,王玉林,沈中毅,殷岫君.金属学报,1997;33:621(Shen D J, Wang Y L, Shen Z Y, Yin X J. Acta Metall Sin, 1997; 33: 621)
4晁月盛,滕功清,谢春辉,耿岩,赖祖涵.金属学报.1996;32: 1204(Chao Y S,Teng G Q,Xie C H,Geng Y,Lai Z H. Acta Metall Sin,1996; 32:1204)
5Luborsky P E, Walter J L.J Appl Phgs, 1976 47: 3648
6Gerling R,Schimansky F P,Wagner R.Int J Rapid Solidif,1990; 5:137
7Chen H S. J Appl Phys, 1978; 49: 3289
8KroegerD M,Canright G S,MaKamey CG,Easton D S,Scarbrough J O.Acta Metall,1987;35:989
9Liebermann H H, Marti J, Martis R J, Wong C P. Metall Trans, 1989; 20A: 63i
[1] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
[4] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[5] WANG Xiaobo, WANG Yongzhe, CHENG Xudong, JIANG Rong. Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air[J]. 金属学报, 2021, 57(3): 327-339.
[6] PENG Yanyan, YU Liming, LIU Yongchang, MA Zongqing, LIU Chenxi, LI Chong, LI Huijun. Effect of Ageing Treatment at 650 ℃ on Microstructure and Properties of 9Cr-ODS Steel[J]. 金属学报, 2020, 56(8): 1075-1083.
[7] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[8] Jianxiong ZOU,Bo LIU,Liwei LIN,Ding REN,Guohua JIAO,Yuanfu LU,Kewei XU. Microstructure and Thermal Stability of MoC DopedRu-Based Alloy Films as Seedless Diffusion Barrier[J]. 金属学报, 2017, 53(1): 31-37.
[9] Weiwei GUO,Chengjun QI,Xiaowu LI. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN CONJUGATE AND CRITICAL DOUBLE-SLIP-ORIENTED Cu SINGLE CRYSTALS[J]. 金属学报, 2016, 52(6): 761-768.
[10] YANG Bin, LI Xin, LUO Wendong, LI Yuxiang. EFFECT OF MINOR Sn AND Nb ADDITIONS ON THE THERMAL STABILITY AND COMPRESSIVE PLASTICITY OF Zr-Cu-Fe-Al BULK METALLIC GLASS[J]. 金属学报, 2015, 51(4): 465-472.
[11] LIU Wenbo, ZHANG Chi, YANG Zhigang, XIA Zhixin, GAO Guhui, WENG Yuqing. EFFECT OF SURFACE NANOCRYSTALLIZATION ON MICROSTRUCTURE AND THERMAL STABILITY OF REDUCED ACTIVATION STEEL[J]. 金属学报, 2013, 49(6): 707-716.
[12] ZHANG Lidong, WANG Fei, CHEN Shunli, WANG Yuan. FABRICATION AND THERMAL STABILITY OF AlCrTaTiNi/(AlCrTaTiNi)N BILAYER DIFFUSION BARRIER[J]. 金属学报, 2013, 49(12): 1611-1616.
[13] FANG Lu,DING Xianfei, ZHANG Laiqi, HAO Guojian, LIN Junpin. MICROSTRUCTURE STABILITY IN A FULLY LAMELLAR HIGH Nb-TiAl ALLOY AFTER LONG-TERM THERMAL CYCLING[J]. 金属学报, 2013, 49(11): 1416-1422.
[14] ZHANG Yanpo, REN Ding, LIN Liwei,YANG Bin, WANG Shanling,LIU Bo1), XU Kewei. CONTROLLED REACTION ON INTERFACE OF Cu/Cu(Ge, Zr)/SiO2/Si MULTILAYER FILM AND ITS THERMAL STABILITY[J]. 金属学报, 2013, 49(10): 1264-1268.
[15] GUO Weiwei, QI Chengjun, LI Xiaowu. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN A DOUBLE-SLIPORIENTED Cu SINGLE CRYSTAL[J]. 金属学报, 2013, 49(1): 107-114.
No Suggested Reading articles found!