| STUDY ON THE FLUX IN STEEL-ALUMINIUM SOLID TO LIQUID BONDING |
| ZHANG Peng; CUI Jtanzhong; DU Yunhui (Northeastern University; Shenyang 110006); BA Limin (Anshan Aulomobile Fittings Factory; Anshan 114014) (Manuscript received 1996-06- 19; in revised form 1997-02-26) |
|
Cite this article:
ZHANG Peng; CUI Jtanzhong; DU Yunhui (Northeastern University; Shenyang 110006); BA Limin (Anshan Aulomobile Fittings Factory; Anshan 114014) (Manuscript received 1996-06- 19; in revised form 1997-02-26). STUDY ON THE FLUX IN STEEL-ALUMINIUM SOLID TO LIQUID BONDING. Acta Metall Sin, 1997, 33(8): 869-873.
|
|
|
Abstract This paper studied the effect of the welding-supporting technology on the quality of steel-aluminium solid to liquid bonding. The results show that welding-supporting technology can solve interface oxidation problem in the process of solid to liquid bonding, and interfacial strength in steel-aluminium solid to liquid bonding could increase substantially by immersing flux No.1 made up with halogenide.
|
|
Received: 18 August 1997
|
1段世铎,高广利编.界面化学.北京:高等教育出版社,1993:63 2倪红军.特种铸造及有色合金,1994;5:29 3斋藤好弘,小林英雄.平成5年度塑性加工春季讲演会, 1993 4钱卫江.材料工程, 1994; 8-9:13 5张鹏,崔建忠,杜云慧.金属学报,1996;32:1275 6张折衷.无机物手册.北京:科学教育出版社,1986:48 7华勤学.机械工程材料, 1995; 19(1): 23 8顾国成,刘帮津.热浸镀.北京:化学工业出版社,1994: 76 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|