MAGNETIC,MAGNETO-OPTICAL PROPERTIES AND THERMAL STABILITY OF Tb/Co MULTILAYER FILMS
ZOU Zhiqiang;LI Ming;JIANG ZhihonK;LUO Caiqing; SHEN Defang (Shanghai Institute of Metallurgy; Chinese Academy of Sciences; Shanghai 200050)
Cite this article: 

ZOU Zhiqiang;LI Ming;JIANG ZhihonK;LUO Caiqing; SHEN Defang (Shanghai Institute of Metallurgy; Chinese Academy of Sciences; Shanghai 200050). MAGNETIC,MAGNETO-OPTICAL PROPERTIES AND THERMAL STABILITY OF Tb/Co MULTILAYER FILMS. Acta Metall Sin, 1997, 33(7): 749-755.

Download:  PDF(661KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Tb/Co thin films with an artificially layered structure are prepared by a dc magnetron-sputtering system. The form of the compositionally modulated structure is dependent on the deposition rates of Tb and Co targets, and the rotation speed of substrate. The layer-thickness dependence of Kerr rotation hysteresis loops was studied. The results show that the films have large pefpendicular uniaxial anisotropy, large coercivity and large Kerr rotation when the period of Tb/Co film is small. These magnetic properties decrease when the period of Tb/Co film is large. The mechanism can be interpreted in terms of the single-ion anisotropy of Tb ions in the interface, and the ferrimagnetic coupling between Tb and Co atoms. The isothermal annealing of Tb/Co multilayer films at 300 oC shows that it has a bad thermal stability.
Key words:  Tb/Co compositionally modulated film      perpendicular anisotropypeerr rotation angle      thermal stability     
Received:  18 July 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I7/749

1KrishnanR,Cagan V,PorteM,TessierM.J Magn Magn Mater,1990;83:65
2 Sato N,HabuK.JApdPhyS,1987;61:4287Sato N, Habu K, Oyama T. IEEE Trans Mop, 1987; MAG23: 2614
3 SatoN.J Appl Phys,1986;59:2514
4Shan Z S, Sellmyer D J. J Appl Phys, 1999; 67: 5713
Shan Z S, Sellmyer D J. J Appl Phys, 1988; 64. 5745
5 Wang Y J, Kleemann W. Phys Rev, 1991, B44: 5132
6 Shen D F, Jin L N, Yu X Y, Wang L J. J Rare Earths, 1992; 4: 288
7 Morishita T, Togami Y, Tsushima K. J Phys Soc Jpe, 1985; 54. 37
8 Landau L D, Lifshitz E M. Electrodynamics of Continous Medta. London: Pergamon, 1984: 3319 Zwingnan R, Wilson W L, Bourne H C. AIP COnfProc, 1976; 34. 334
10 Suzuki Y, Takayama S, Kirino F, Ohta N. IEEE Trans Magn, 1987, MAG-23t 2275
11 Meiklejohn W H, Luborsky F E, Frishchman P G. IEEE Trans Mag, 1987; MAG-23. 2272
12 Shan Z S, Sellmyer D J, Jaswal S S, Wang Y J, Shen J X. Phys Rev Lelt, 1989; 63: 449
Shan Z S, Sellmyer D J, Jaswal S S, Wang Y J, Shen J X. Phys Rev, 1990; B42: 10446
13 Luborsky F E, Furey J T, Skoda R E, Wagner B C. IEEE Trans Magn, 1985; MAG-21: 1618
[1] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
[4] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[5] WANG Xiaobo, WANG Yongzhe, CHENG Xudong, JIANG Rong. Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air[J]. 金属学报, 2021, 57(3): 327-339.
[6] PENG Yanyan, YU Liming, LIU Yongchang, MA Zongqing, LIU Chenxi, LI Chong, LI Huijun. Effect of Ageing Treatment at 650 ℃ on Microstructure and Properties of 9Cr-ODS Steel[J]. 金属学报, 2020, 56(8): 1075-1083.
[7] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[8] Jianxiong ZOU,Bo LIU,Liwei LIN,Ding REN,Guohua JIAO,Yuanfu LU,Kewei XU. Microstructure and Thermal Stability of MoC DopedRu-Based Alloy Films as Seedless Diffusion Barrier[J]. 金属学报, 2017, 53(1): 31-37.
[9] Weiwei GUO,Chengjun QI,Xiaowu LI. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN CONJUGATE AND CRITICAL DOUBLE-SLIP-ORIENTED Cu SINGLE CRYSTALS[J]. 金属学报, 2016, 52(6): 761-768.
[10] YANG Bin, LI Xin, LUO Wendong, LI Yuxiang. EFFECT OF MINOR Sn AND Nb ADDITIONS ON THE THERMAL STABILITY AND COMPRESSIVE PLASTICITY OF Zr-Cu-Fe-Al BULK METALLIC GLASS[J]. 金属学报, 2015, 51(4): 465-472.
[11] LIU Wenbo, ZHANG Chi, YANG Zhigang, XIA Zhixin, GAO Guhui, WENG Yuqing. EFFECT OF SURFACE NANOCRYSTALLIZATION ON MICROSTRUCTURE AND THERMAL STABILITY OF REDUCED ACTIVATION STEEL[J]. 金属学报, 2013, 49(6): 707-716.
[12] ZHANG Lidong, WANG Fei, CHEN Shunli, WANG Yuan. FABRICATION AND THERMAL STABILITY OF AlCrTaTiNi/(AlCrTaTiNi)N BILAYER DIFFUSION BARRIER[J]. 金属学报, 2013, 49(12): 1611-1616.
[13] FANG Lu,DING Xianfei, ZHANG Laiqi, HAO Guojian, LIN Junpin. MICROSTRUCTURE STABILITY IN A FULLY LAMELLAR HIGH Nb-TiAl ALLOY AFTER LONG-TERM THERMAL CYCLING[J]. 金属学报, 2013, 49(11): 1416-1422.
[14] ZHANG Yanpo, REN Ding, LIN Liwei,YANG Bin, WANG Shanling,LIU Bo1), XU Kewei. CONTROLLED REACTION ON INTERFACE OF Cu/Cu(Ge, Zr)/SiO2/Si MULTILAYER FILM AND ITS THERMAL STABILITY[J]. 金属学报, 2013, 49(10): 1264-1268.
[15] GUO Weiwei, QI Chengjun, LI Xiaowu. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN A DOUBLE-SLIPORIENTED Cu SINGLE CRYSTAL[J]. 金属学报, 2013, 49(1): 107-114.
No Suggested Reading articles found!