MUTUAL SEPARATION OF RARE EARTH CHLORIDE MIXTURES USING A DRY PROCESS |
YU Jin (Shenyang Polytechnic University; Shenyang 110023) YU Yongli; WANG Zhichang (Northeastern University; Shenyang 110006)(Manuscript received 1996-04-03) |
|
Cite this article:
YU Jin (Shenyang Polytechnic University; Shenyang 110023) YU Yongli; WANG Zhichang (Northeastern University; Shenyang 110006)(Manuscript received 1996-04-03). MUTUAL SEPARATION OF RARE EARTH CHLORIDE MIXTURES USING A DRY PROCESS. Acta Metall Sin, 1997, 33(4): 391-394.
|
Abstract Mutual separation of neighboring rare earth elements has been investigated from their binary chloride mixtures LaCl3-CeCl3, CeCl3-PrCl3, PrCl3-NdCl3 and their quaternary chloride mixtures LaCl3-CeCl3-PrCl3-NdCl3 by using a dry process (i.e. chemical vapour transport process), in which the aluminium chloride is selected as complex former.The separation factors from the binary chloride mixtures are 12.3 for La : Ce, 5.79 for Pr:Ce and 1.32 for Pr: Nd. An higher separation factor of Pr:Nd=1.98 was also observed from their quaternary chloride mixture.
|
Received: 18 April 1997
|
1Jacobs R S,Krupke W F,Hessler J P,Carnall W T.Opt Commun,1977;2:395 2Jacobs R R,Krupke W F. Appl Phys Lett,1978;32:3,1979;35:126 3Caird J A,Carnall W T,Hesslor J P,Williams C W. J Chem Phys,1981;74:798 4Hake D,Urland W,Kremer R.Z Anorg Chem,1987;550:35 5Hake D,Urland W. Z Anorg Chem,1990;586:99 6Murase K,Machida K,Adachi G.Chem Lett,1992:1555 7Murase K,Machida K,Adachi G.J Alloys Comp,1991;217:218 8Adachi G,Shinozaki K,Hirashima Y,Machida K.J Less-Common Met,1992 169:L1 9Adachi G,Murase K,Shinozaki K,Machida K. Chem Lett,1992;511 10Murase K,Shinozaki K,Machida K,Adachi G. Bull Chem Soc Jpn,1992;65:2724 11Murase K,Shinozaki K,Hirashima Y,Machida K,Adachi G.J Alloys Comp,1993;198:31h |