HYDROGEN INDUCED-IN DEFECT AND RECOVERY BEHAVIOUR IN POLYCRYSTALLINE NICKEL
ZHAO Faru; WANG Baoyi (Lanzhou University; Lanzhou 730000); TONG Zhichen (Shanghai Mechanical Engineering Collnge; Shanghai 200040); WANG Tianmin (Lanzhou University; Lanzhou 730000;Lanzhou Institute of Chemistry-Physics;Chinese Academy of Sciences; Lanzhou 730000)(Manuscript received 1996-05-10; in revised form 1996-1 1-27)
Cite this article: 

ZHAO Faru; WANG Baoyi (Lanzhou University; Lanzhou 730000); TONG Zhichen (Shanghai Mechanical Engineering Collnge; Shanghai 200040); WANG Tianmin (Lanzhou University; Lanzhou 730000;Lanzhou Institute of Chemistry-Physics;Chinese Academy of Sciences; Lanzhou 730000)(Manuscript received 1996-05-10; in revised form 1996-1 1-27). HYDROGEN INDUCED-IN DEFECT AND RECOVERY BEHAVIOUR IN POLYCRYSTALLINE NICKEL. Acta Metall Sin, 1997, 33(4): 345-351.

Download:  PDF(643KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Specimens made of fully annealed or plastically deformed polycrystalline nickel are hydrogen charged. The properties and recovery behaviour of the hydrogen induced defects are studied by means of positron annihilation. The measured activation energy for migration of a vacancy is 0.96±0.05 eV. The results showed that both for the fully annealed and plastically deformed polycrystalline nickel, the parameter S and the average lifetime will increase sharply when the specimens were hydrogen charged. The type of the hydrogen charged defects depends on the state of the specimen before charging, in a fully annealed specimen, except some of vacancies and dislocations, the main hydrogen charged defects are the micro voids or the micro cracks, which can not be recovered at above 650℃. Compared with the annealed samples, the hydrogen induced defects are mainly vacancies, dislocations and vacancy clusters, and the microvoids was not found in the deformed nickel specimen.
Key words:  hydrogen charging      positron annihilation      polycrystalline nickel      micro defect     
Received:  18 April 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I4/345

1Wert C A.In:Alfeld G,Volkl J eds,Hydrogen in Metals.Heidelberg:Springer-Verlag,1978:305
2藤田英一.金属中水素,日本金属学会会报,1979;18(9):613
3Lee S M,Lee J Y.Metall Trans,1986;17A:181
4Szdes C,Lang G,Kajcsos Z.Mater Sci Forum,1992;105-110:1261
5Lee J L,Lee J Y.Ser Metall,1985;19:341
6吴奕初,田中卓.常香荣,肖纪美。物理学报,1991;40(11):1883
7Khanna S K,Sonnenberg K.Radiat Eff, 1981;59:91
8Dlubek G,Brummer O,Hensel E.Phys Status Solidi,1976;34A:737
9Siegel R W,In:Takamura J I,Doyama M,Kiritani M eds,Point Defects and Defect Interactions inMetals.Tokyo:University of Tokyo Press,1982:533
10王天民.核技术,1987;4:7
11Pajak J,Rozenfeld B.In:Jain P C,Singru R M,Gopinathan K P eds.,Positron Annihilation,Singapore:World Scientific Publ Co,1985:558
12Segers D,Humbeeck J V,Delaey L, Dorikens M.In:Jain P C,Singru R M,Gopinathan K P eds.,Positron Annihilation,Singapore:World Scientific Publ Co,1985:880
13高飞,赖文生,王天民。兰州大学学报(自然科学版),1993;29(1):54
14Wang B Y,Gu Q,Wang Y X,Wang T M. J Phys. F,to be published
15冯端。金属物理学(第一卷:结构与缺陷)北京:科学出版社,1987:308
16Trumpy G,Bentzon M. Mater Sci Forum,1992;105-110:1293
[1] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[2] TIAN Xuefen, LIU Xiang, GONG Min, ZHANG Peiyuan, WANG Kang, DENG Aihong. Defect Evolution in H/He Neutral Beam Irradiated W-ZrC Alloy Using Positron Annihilation Spectroscopy[J]. 金属学报, 2021, 57(1): 121-128.
[3] Tianci ZHANG, Haitao WANG, Zhengcao LI, Henk SCHUT, Zhengming ZHANG, Ming HE, Yuliang SUN. Positron Annihilation Investigation of Embrittlement Behavior in Chinese RPV Steels after Fe-Ion Irradiation[J]. 金属学报, 2018, 54(4): 512-518.
[4] Kang WANG,Aihong DENG,Min GONG,Xiaobo LU,Yuanyuan ZHANG,Xiang LIU. Effect on Microstructure of Tungsten Under Helium Ions Irradiation with Multiple Energy[J]. 金属学报, 2017, 53(1): 70-76.
[5] Pingguang XU,Jiang YIN,Shuyan ZHANG. TENSILE DEFORMATION BEHAVIOR OF HYDROGEN CHARGED ULTRAHIGH STRENGTH STEEL STUDIED BY IN SITU NEUTRON DIFFRACTION[J]. 金属学报, 2015, 51(11): 1297-1305.
[6] LIU Yang, XIANG Wei, WANG Boyu. EFFECT OF IRRADIATION WITH PULSED ION BEAM ON THE MICROSTRUCTURE OF TiH2[J]. 金属学报, 2013, 49(10): 1269-1274.
[7] WANG Xiaoyong, PAN Tao, WANG Hua, SU Hang,LI Xiangyang, CAO Xingzhong. INVESTIGATION OF THE TOUGHNESS OF LOW CARBON TEMPERED MARTENSITE IN THE SURFACE OF Ni-Cr-Mo-B ULTRA-HEAVY PLATE STEEL[J]. 金属学报, 2012, 48(4): 401-406.
[8] WANG Boyu XIANG Wei TAN Xiaohua DAI Jingyi CHENG Liang QIN Xiubo. EFFECT OF D+ BEAM IRRADIATION ON Ti FILM[J]. 金属学报, 2010, 46(7): 810-813.
[9] ZHANG Lanzhi; WANG Baoyi; WANG Danni; WEI Long; LIN Junpin; WANG Wenjun. STUDIES OF Nb–TiAl ALLOY BY POSITRON ANNIHILATION TECHNIQUES[J]. 金属学报, 2007, 43(3): 269-272 .
[10] Jian Zhang. STUDY OF HYDROGEN EMBRITLLEMENT IN Fe-Ni BASED ALLOY THROUGH POSITRON ANNIHILATION LIFETIME TEST[J]. 金属学报, 2006, 42(5): 469-473 .
[11] DENG Wen; RUAN Xiangdong; HUANG Yuyang; ZHOU Yin'e; ZHU Yingying; ZHU Yingying. Effects Of Twin Size On The Dislocation Configuration During Cyclic Deformation Of Polycrystalline Twin Copper[J]. 金属学报, 2005, 41(1): 33-.
[12] JIA Wei;XIONG Lianggue;ZENG Meiguang;WANG Jiangiang (Department of Materials Science; College of Science; Northeastern University; Shenyang 110006)(International Center for Materials Physics; Institute of Matal Research; The Chinese Academy of Sciences;Shenyang 110015). POSITRON ANNIHILATION STUDY ON THE EFFECT OF MISCH METAL IN Al-Fe-V-Si-Mm ALLOYS[J]. 金属学报, 1998, 34(2): 221-224.
[13] XIONG Liangyue1;2); CHEN Jian1); HU Zhuangqi1)(Institute of Metal Research; Chinese Acdemy of Sciences; Shenyang 110015)(International Center for Materials Physics; Chinese Academy of Sciences;Shenyang 110015). POSITRON LIFETIME SPECTRA OF DUCTILE NiAl-Fe INTERMETALLIC ALLOYS[J]. 金属学报, 1996, 32(11): 1189-1193.
[14] GU Yuefong; DENG Wen; GUO Jianting; (Institute of Meial Research; Chinese A cademy of Sciences; Shenyang 110015)XIONG Liangyue; LIN Dongliang (Institute of Metal Research; Chinese A cademy Sciences. Shenyang 110015)(Shanghai Jiaoiong University; Shanghai 200030). PAT STUDY OF EFFECT OF Zr ON DEFECTS IN Ni_3Al ALLOY[J]. 金属学报, 1995, 31(17): 238-240.
[15] LIU Tao; PU Yuxie; ZHAO Zhongtao; MA Ruzhang(University of Sciene and technology Beijing; 100083). GUO Yinghuan(Institute of High Energy Physics;Chinese Academiy of Sciences;Beijing 1000800)(Manuscript received 1994-07-11;in revised form 1994-12-01). STRUCTURAL DEFECT AND INTERNAL STRESS ARRANGEMENT IN NANOCRYSTALLINE Fe73.5Cu1Nb3Si13.5B9[J]. 金属学报, 1995, 31(16): 159-163.
No Suggested Reading articles found!