Acta Metall Sin  1997, Vol. 33 Issue (4): 337-344    DOI:
Current Issue | Archive | Adv Search |
NUMERICAL SIMULATION ON RING COMPRESSION──A New Approch to Determine Calibration Curves of Friction Coefficient
HU Zhong; ZHU Lihua; LI Jiaqing (Tsinghua University;Beijing100084)(Manuscript received 1996-04-05; in revised form 1996-06-06)
Cite this article: 

HU Zhong; ZHU Lihua; LI Jiaqing (Tsinghua University;Beijing100084)(Manuscript received 1996-04-05; in revised form 1996-06-06). NUMERICAL SIMULATION ON RING COMPRESSION──A New Approch to Determine Calibration Curves of Friction Coefficient. Acta Metall Sin, 1997, 33(4): 337-344.

Download:  PDF(614KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  This paper describes the theory of elasto-plastic FEM for large strain and themathematical model of the contact problems on the dynamic boundary. And it presents thesimulation results of the ring compression by using the elasto-plastic FEM program ANSYS 5.1 and the material constitutive relationship in hot metal working. The theoretical calibration curves of determining the friction coeffcient for 6:3:2 rings have been predicted.The equivalent strain and theshear stress distributions have been presented.
Key words:  ring compression      friction coeffcient      elasto-plasticFEM      metal forming     
Received:  18 April 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I4/337

1范钦之.清华大学硕士学位论文,1981
2胡忠.塑性工程学报,1994;1(3):3
3杨军,皇甫骅。锻压技术,1991;(4):10
4周纪华,管克智.金属塑性变形阻力.北京:机械工业出版社,1989:9
5Pawelski O,et al.Steel Res,1989;60(9):395
6Lee C H,Altan T. Trans ASME,J Eng Ind,1972;94:775
7Meng Y, Hiroyuki S.In:Wang Z R,He Yuxin eds.Proceeding of 4th International ConferenceonTechnology of Plasticity.Beijing:International Academic Publishers,1993:1169
[1] WANG Peng DONG Xianghuai FU Lijun. MULTI-STEP NUMERICAL SIMULATION OF BULK METAL FORMING PROCESSES BASED ON DEFORMATION THEORY OF PLASTICITY[J]. 金属学报, 2009, 45(1): 124-128.
[2] HAN Jingtao (University of Science and Technology Beijing; Beijing 100083);ZHAO Gang (The 1202 Factory of PLA; Beijing 100036); CAO Qixiang(Tsinghua University; Beijing 100084) (Manuscript received 1995-11-10; in revised form 1996-02-14). DISCOVERY OF INNER CRACK RECOVERY AND ITS STRUCTURE CHANGE IN 20MnMo STEEL[J]. 金属学报, 1996, 32(7): 723-729.
No Suggested Reading articles found!