Abstract  Geometrical model is a kind of solution model that has been used extensively in predicting thermodynamic properties and calculating phase diagrams for ternary and multicomponent systems. However, all current geometrical models have their inherent defects since they have improperly assumed that the models are independent of the system treated. In order to overcome these inherent defects that lasted for almost 30 years, a complete new assumption has been given, that is, the selected model should be closely related to the systems considered. After a new conception "similarity coefficient" has been introduced, a new geometrical model has been established that can overcome all defects appearing in the current models. We call this kind of models as a new generation model. In this paper the problems for this kind of model and the possible development have also been discussed.
Key words:  thermodynamics      solution model      phase diagram      multicomponent system     
Received:  18 February 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I2/126

1 Kohler Monatsh.Chem, 1960; 91:738
2 Bonnier E Caboz R.Compt,Rend, 1960; 250:527
3 Toop G W.Trans AIME 1965;233: 850
4 Colinet C,D.E.S, Fac Sci,Univ Grenoble,France,(1967)
5 Muggianu Y M,Gambino M,Bros J-P.J Chim Phys(Paris),1965;72:83
6 Jacob K J, Fitzner K. Thermochim Acta, 1973; 18:197
7 Ansaral Int Met Rev,1979 (1): 20
8 Hillert M.CALPHAD 1980; 4(1):1
9 Luck L,Gening U, Predel B. Z Metalkde,1986; 77: 442
10 周国治. 全同第四届熔盐化学和电化学会议文集、郑州,1987
11 Chou K C. CALPHAD, 1987;11(2):123
12 李瑞青,北京科技人学硕士学位论文,1988
13 Chen S L, Chou K C.Rare Met,1989; 8(4): 22
14 Chou K C, Li R Q.Rare Met, 1989;8(4):12
15 Li R Q.CALPHAD, 1989;13(1):67
16 Chen S L,Chou K C. CALPHAD, 1989 13(1):79
17 Chen S L,Cui J Q.Chen T K,Chou K C.CALPHAD,1989; 13(3):225
18 Chou K C, Chang Y A Ber Bunsen-Ges Phys Chem, 1989 93: 741
19 Chou K C.J General Geometrical Model, CALPHAD XXIII-CAMSE 94,Madison,Wisconsin,USA, 1994
20 Chou K C. A New Solution Model For Predicting Thermodynamic Properties of Multicompouent System From Binaries, CALPHAD XXIV95,Kyoto,1995
21 Chou K C. CALPHAD,1995;19(3):315
22 Chou K C et al.Metall Mater Trans.(to be published)
[1] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[2] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[3] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[4] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[5] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[6] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[7] Liheng LIU,Chunshan CHE,Gang KONG,Jintang LU,Shuanghong ZHANG. DESTABILIZATION MECHANISM OF Fe-Al INHIBITION LAYER IN Zn-0.2%Al HOT-DIP GALVANIZING COATING AND RELATED THERMODYNAMIC EVALUATION[J]. 金属学报, 2016, 52(5): 614-624.
[8] Feng LIU, Kang WANG. DISCUSSIONS ON THE CORRELATION BETWEEN THERMODYNAMICS AND KINETICS DURING THE PHASE TRANSFORMATIONS IN THE TMCP OF LOW-ALLOY STEELS[J]. 金属学报, 2016, 52(10): 1326-1332.
[9] XIE Jun, YU Jinjiang, SUN Xiaofeng, JIN Tao, SUN Yuan. CARBIDE EVOLUTION BEHAVIOR OF K416B AS-CAST Ni-BASED SUPERALLOY WITH HIGH W CONTENT DURING HIGH TEMPERATURE CREEP[J]. 金属学报, 2015, 51(4): 458-464.
[10] WU Changjun, ZHU Chenlu, SU Xuping, LIU Ya, PENG Haoping, WANG Jianhua. THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. 金属学报, 2014, 50(8): 930-936.
[11] MA Ping, WU Erdong, LI Wuhui, SUN Kai, CHEN Dongfeng. MICROSTRUCTURES AND HYDROGEN STORAGE PROPERTIES OF Ti0.7Zr0.3(Cr1-xVx)2 ALLOYS[J]. 金属学报, 2014, 50(4): 454-462.
[12] WANG Bin, LIU Zhenyu, ZHOU Xiaoguang, WANG Guodong. CALCULATION OF TRANSFORMATION DRIVING FORCE FOR THE PRECIPITATION OF NANO-SCALED CEMENTITES IN THE HYPOEUTECTOID STEELS THROUGH ULTRA FAST COOLING[J]. 金属学报, 2013, 49(1): 26-34.
[13] LI Wuhui TIAN Baohong MA Ping WU Erdong. HYDROGEN STORAGE PROPERTIES OF ScMn2 ALLOY[J]. 金属学报, 2012, 48(7): 822-829.
[14] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[15] WU Chaofeng MA Mingxing WU Aiping LIU Wenjin ZHONG Minlin ZHANG Weiming ZHANG Hongjun. MORPHOLOGIC CHARACTERISTICS OF IN SITU SYNTHESIZED CARBIDE PARTICLES IN LASER CLADDED Fe-BASED COMPOSITE COATINGS[J]. 金属学报, 2009, 45(9): 1091-1098.
No Suggested Reading articles found!