EFFECT OF Nb AND Ti CONTENTS ON MICRO-SEGREGATION OF J-90 ALLOY
WANG Anchuan; LI Yiyi; LI Dongfa; YANG Ke; FAN Cungan; SHI Changxu(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

WANG Anchuan; LI Yiyi; LI Dongfa; YANG Ke; FAN Cungan; SHI Changxu(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). EFFECT OF Nb AND Ti CONTENTS ON MICRO-SEGREGATION OF J-90 ALLOY. Acta Metall Sin, 1995, 31(5): 216-222.

Download:  PDF(595KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  EMPA has been performed to investigate the distribution of Nb and Ti in the solidification structure of J-90 alloys with different contents of Nb and Ti. With increasing of Nb content in the alloy, Nb tends to be seriously segregated, while distribution of Ti becomes more and more homogeneous, but when the content of Ti in the alloy being increased, segregations of Nb and Ti are all lessened. By increasing contents of Nb and Ti in the alloy, partition coefficients of Nb and Ti at the beginning of solidification are all increased. It was found by comparison that difference between the highest and the lowest content of an element after solidification is a more proper parameter for description of elemental segregation which is dependent on the content of elements and the elemental partition coefficient. The fact that k_(Nb) and k_(Ti) increased with increasing of Nb and Ti contents in the alloys indicated that when contents of trace elements (such as P etc.) were lowered, on the solute-rich layer during solidification there would be less these trace elements while contents of easy-segregated elements, such as Nb and Ti, could increased. As a consequence, k_(Nb) and k_(Ti) would increase and micro-segregation of Nb and Ti would decrease.
Key words:  Nb      Ti      J-90 alloy      micro-segregation     
Received:  18 May 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I5/216

1高温合金组,中国科学院金属研究所内部资料,19852AlloyDigest,FilingCode:Fe-83,February,19883AlloyDigest.FilingCode:Fe-50,January,19744王安川,范存淦,李冬法,李依依.中国科学院金属研究所内部资料,19935WangAnchuan,YangKe,LIYiyi.2ndIntConfonInteractionofSteelswithHydrogeninPetroleum,IndustryPressureVesselandPipelineService,October,19-21,1994,Vienna,1994:5136NakkalilR,RichardsNL,ChaturvediMC.ScrMetallMater,1992:26:5457FlemmingsMC.SolidificationProcessing.Chapter2,NewYork:McGraw-Hill,19748BattleTP,PehlkeRD.Metalltrans,1989;20B:149
[1] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[2] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[3] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[6] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[7] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[8] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[9] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[10] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[11] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[12] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[13] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[14] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[15] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
No Suggested Reading articles found!