Abstract The in situ tensile test under TEM for thin foil specimen of brass showed that a lot of dislocations could be emitted from a loaded crack tip and a dislocation free zone(DFZ) could form after reaching equilibrium. The DFZ was a nonlinearly elastic zone with large strain(ε≈0. 1) and the stress in the DFZ might equal to the cohesive strength σ_(th) when the crack tip was sharp enough and an applied stress was large enough. As a result, a nanocrack initiated discontinuously in the DFZ or sometimes at a blunted-crack tip. As soon as the nanocrack nucleated, it would quickly blunt into a void even under keeping constant displacement.
|
|
Received: 18 August 1994
|
| 1WilsdorfHGF.MaterSciEng,1983;59:12OhrSM,MaterSciEng,1985;72:13姚可夫,唐乃泳,陈南平.金属学报,1989;25:A213姚可夫,唐乃泳,陈南平.金属学报,1991,27:A984黎晶,张统一,褚武扬,肖纪美.金属学报,1988;24(SupplⅡ):SA1345陈奇志,褚武扬,肖纪美.中国科学,1994;A24:2916张跃,王燕斌,褚武扬,肖纪美.中国科学,1994;A24(6)7高克玮,陈奇志,褚武扬,肖纪美.中国科学,待发表8Hirschp,HowieA,NicholsonRB,PashleyDW,WhelanMJ,ElectronMirceoscopyofThinCrystals.2nded,Huntington:RobertE.KriegerPubCo.,1977:3649HirthJP,LotheJ.TheoryofDistocations,2nded,NewYork:Wiley,1982:23010ThomsonAW,KnottJF,MetallTrans,1993;24A:52311重有色金属材料加工手册.北京:冶金工业出版社,1979:7012WeertmanJ,LinIH,ThomsonR.ActaMetall.1983;31:47313褚武扬.断裂力学基础.北京:科学出版社,1979:11614CherepanovGP.MechanicsofBrittleFracture.NewYork:McGraw-Hill,1979:29 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|