A TEM STUDY OF SPINODAL DECOMPOSITION IN Fe-1 .83C MARTENSITE |
REN Xiaobing; WANG Xiaotian (Xi'an Jiaotong University) SHIMIZU Ken'ichi(Kanazawa institute of Technology; Japan) TADAKI Tsugio (Osaka University;Japan)(Manuscript received 27 October; 1993; in revised form 4 January; 1994) |
|
Cite this article:
REN Xiaobing; WANG Xiaotian (Xi'an Jiaotong University) SHIMIZU Ken'ichi(Kanazawa institute of Technology; Japan) TADAKI Tsugio (Osaka University;Japan)(Manuscript received 27 October; 1993; in revised form 4 January; 1994). A TEM STUDY OF SPINODAL DECOMPOSITION IN Fe-1 .83C MARTENSITE. Acta Metall Sin, 1994, 30(7): 289-295.
|
Abstract Diffuse scattering and microstructure of Fe-1.83C(%) martensite aged at room temperature was studied by TEM. The intensity distribution of diffuse scattering in reciprocal space was determined by double-tilt technique. The results show that the shape of martensite diffraction spot becomes a diffuse spike after aging, and its 3-dimensional profile appears to be two head-on 4-sided regular pyramids. Fourier analysis of the diffuse scattering suggests that martensite undergoes a spinodal decomposition during aging,the tweed-like modulated structure is composed of a dominant wave with wavelength of about 1 nm and non-dominant waves with longer wavelengths. For the first time it is found that the modulated structure of Fe-C martensite does not grow even after aged for several months.The reason is considered to be due to the strong elastic interactions among carbon-enriched and depleted regions.Correspondent: REN Hiaobing, Presently with Department of Physics, Nanjing, University, Nanjing 21008)
|
Received: 18 July 1994
|
1OlsonGB,CohenM.MetallTrans,1983;14A:10572NagakuraS,HirotsuY,KusunokiM,NakamuraY.MetallTrans,1983;14A:10253KusunokiM,NagakuraS.JApplCrystallogr,198l:14:3294TaylorKA,ChangL,OlsonGB,SmithGDW,CohenM,VanderSandeJB.MetallTrans,1989;20A:27175UwakwehONC,GeninJMRR,SilvainJG.MetallTrans,1991;22A:7976KhachaturyanAG.TheoryofStructuralTransformationsinSolide.JohnWiley&Sons,19837CahnJW.ActaMetall,1961;9:5258CahnJW.ActaMetall.1961;9:7959RenSB,WangST.MetallTrans,1988;19A:242710任晓兵,王笑天.金属热处理学报,1990;11:2811KhachaturyanAG,OnishimovaTA.PhysMetMetallogr,1968;26:1212LangerJS,Bar-onM,MillerHD.PhysRev,1975:A11:141713MiyazakiT,DoiM.MaterSciEng,1989;A110:17514KawasakiK,EnomotoY.Physica,1988;A150:46 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|