| TRANSFORMATION KINETICS AND COARSENING OF LAMELLAR STRUCTURE IN γ-TiAl ALLOY |
| TIAN Huahang;HUANG Zheng;CHEN Changqi(Beijing University of Aeronautics and Astronautics); LIN Jianguo(University of Xiang tan)(Manuscript received 5 April;1993;in revised form 28 September;1993) |
|
Cite this article:
TIAN Huahang;HUANG Zheng;CHEN Changqi(Beijing University of Aeronautics and Astronautics); LIN Jianguo(University of Xiang tan)(Manuscript received 5 April;1993;in revised form 28 September;1993). TRANSFORMATION KINETICS AND COARSENING OF LAMELLAR STRUCTURE IN γ-TiAl ALLOY. Acta Metall Sin, 1994, 30(3): 117-123.
|
|
|
Abstract Transformation mechanism and discontinuous coarsening of lamellar structure were studied by cooling Ti-47.8at.-%Al alloy fromα region to room temperature and then aging in the two phase region.The lamellar transformation process relates to aging temperature and cooling rate,at which α_2 single phase forms. A model of lamellar transformation kinetics was developed.The stability of lamellae decreases with decreasing interlamellar spacing and discontinuous coarsening occurres during aging.Correspondent:TIAN Huahang,assistant,Laboratory No.8,Department No.1,Beijing University of Aeronautics and Astronautics,Beijing 100083
|
|
Received: 18 March 1994
|
| 1YamabeY,KikuchiM.BullJpnInstMet,1991;30:372YamabeY,HonjoN,KikuchiM.In:lzumiOed.,Proc6thJapanInstituteofMetalsInternationalSymposiumonIntermetallicCompounds(JIMIS-6),Sendali,1991:8213 D.SimonShong,KimY-w.ScrMetall,1989;23:257 4KikuchiM,YamabeY.In:IzumiOed.,Proc6thJapanInstituteofMetalsInternationalSymposiumonIntermetallicCompounds(JIMIS-6),Sendai,1991:8155徐祖耀.相变原理,北京:科学出版社,1988:3316KimY-W.In:JohnsonLA,PopeDP,StieglerJOeds.,HighTemperatureOrderedIntermetallicAlloysⅣ,M.R.S.,Pittsburgh,Pa,1991:7777OuchiK,IijimaY,HiranoKIn:KimuraH,IzumiOeds.,Titanium′80,ScienceandTechnology,TMS-AIME,Warrendale,PA,1980:559 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|