Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (23): 513-518    DOI:
Current Issue | Archive | Adv Search |
SELF-PROPAGATING COMBUSTION REACTION PROCESS OF 45(Ti+C)+55Fe
FAN Quncheng; FANG Xuehua; CHAI Huifen (Xi'an Jiaotong University)(Manuscript received 31 January;1994)
Cite this article: 

FAN Quncheng; FANG Xuehua; CHAI Huifen (Xi'an Jiaotong University)(Manuscript received 31 January;1994). SELF-PROPAGATING COMBUSTION REACTION PROCESS OF 45(Ti+C)+55Fe. Acta Metall Sin, 1994, 30(23): 513-518.

Download:  PDF(510KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A combustion reaction of a compact of 45(Ti+C)+55Fe(wt-%)mixture powders was interrupted by forced cooling so as to maintain the microstructural features revealing the reaction process in the combustion product. Phase compositions and microstructural development in the product were analysed with X-ray diffractometer and scanning electron microscope respectively. Adiabatic temperature, T_ad, was calculated, actual combustion temperature, T_c, and the temperature profile of combuction wave were measured. The results show that the combustion is primarily a solid state reaction which results in a non-simultaneity and incompleteness of the reaction, i. e. TiC particles form first in original Ti powder and then in original Fe powder successively, a small area without TiC particle has been remained within the larger Fe powder.(Correspondent:FAN Quncheng, associate professor, Department of Materials Engineering, Xi'an Jiaotong University, Xi'an 710049)
Key words:  TiC      SHS      reaction process     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I23/513

1VadchenkoSG,Grigor'evYM,MerzhanovAG.CombustExplosShockWaves,1976;12:6062KirdyashkinAI,MaksimovYM,NekrasovEA.CombustExplosShockWaves,1981;17:3773KnyazikVA,MerzhanovAG,SolomonovVB,ShteinbergAS.CombustExplosShockWaves,1985;21:3334NekrasovEA,MaksimovYM,ZiatdinovMK,ShteinbergAS.CombustExplosShockWaves,1978;14:5755AleksandrovVV,KorchaginMA,BoldyrevVV.DokePhysChem,1987;292:1146HoltJB,MunirZA.JMaterSci,1986;21:2517AzatyanTS,Mal'tsevVM,MerzhanovAG,SeleznevVA.CombustExplosShockWaves,1977;13:1568ShkiroVM,BorovinskayaIP.FizikaGoreniaiVzriva,1976;6:9459叶大伦,实用无机物热力学数据手册.北京:冶金工业出版社,198110范群成,柴惠芬,方学华,王笑天.西安交通大学学报,1994;28(7):123P
[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[3] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[4] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[5] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[6] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[7] LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui. A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope[J]. 金属学报, 2023, 59(7): 841-854.
[8] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[9] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[10] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[11] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[12] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[13] XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui. Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing[J]. 金属学报, 2023, 59(5): 693-702.
[14] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[15] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
No Suggested Reading articles found!