INTERFACIAL REACTION IN GRAPHITE FIBRES REINFORCED Al ALLOY COMPOSITES
YANG Haining; GU Mingyuan;JIANG Weiji;ZHANG Guoding(Shanghai Jiaotong University)
Cite this article: 

YANG Haining; GU Mingyuan;JIANG Weiji;ZHANG Guoding(Shanghai Jiaotong University). INTERFACIAL REACTION IN GRAPHITE FIBRES REINFORCED Al ALLOY COMPOSITES. Acta Metall Sin, 1994, 30(20): 379-384.

Download:  PDF(455KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Comparative study under TEM was carried out of the interfacial microstructure in the long graphite fibres reinforced Al-0.35at.-%Ti alloy composites prepared under various conditions. The growth of interfacial reaction product,i.e., Al_4.C_3, was observed under high resolution electron microscope. Results show that the interfaces between the top of Al_4 C_3 and Al alloy matrix are rough and Al_4C_3 grows up continuously, while between the (000l) plane of Al_4C_3 and Al alloy matrix are smooth and Al_4C3 grows up along surfaces. These interfaces have different relative growth rates under differnt growth driving forces.Thus,the morphologies of Al_4C_3 in the composites differ upon the manufacturing parameters were changed. It seems that a proper reduction of volume fraction of graphite fibres will be available to improve further the properties of compsite.
Key words:  composite      interfacial reaction      Al_4C_3      graphite fibre     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I20/379

1KhanIH.Metalltrans,1976;7A:12812YangM,scottVD.JMaterSci,1991;26:16093MarcusHL.AD-A127590,19924MondolfeLF.AluminumAlloys:Structure&Properties.London:Butteeworth,1976:2365闵乃本;晶体生长的物理基础,上海:上海科学技术出版社,1983:4346JeffreyGA,VictorYWu,ActaCrystallogr,1963;16:5597陈荣,上海交通大学博士学位论文,19898BayhaTD,WawnerFE.MetallTrans,1992;23A:1607
[1] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[2] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
[3] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[4] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[5] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[6] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[7] SONG Qingzhong, QIAN Kun, SHU Lei, CHEN Bo, MA Yingche, LIU Kui. Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories[J]. 金属学报, 2022, 58(7): 868-882.
[8] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[9] PAN Chengcheng, ZHANG Xiang, YANG Fan, XIA Dahai, HE Chunnian, HU Wenbin. Corrosion and Cavitation Erosion Behavior of GLNN/Cu Composite in Simulated Seawater[J]. 金属学报, 2022, 58(5): 599-609.
[10] WANG Haowei, ZHAO Dechao, WANG Mingliang. A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites[J]. 金属学报, 2022, 58(4): 428-443.
[11] ZHANG Lei, SHI Tao, HUANG Huogen, ZHANG Pei, ZHANG Pengguo, WU Min, FA Tao. Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites[J]. 金属学报, 2022, 58(2): 225-230.
[12] CHEN Run, WANG Shuai, AN Qi, ZHANG Rui, LIU Wenqi, HUANG Lujun, GENG Lin. Effect of Hot Extrusion and Heat Treatment on the Microstructure and Tensile Properties of Network Structured TiBw/TC18 Composites[J]. 金属学报, 2022, 58(11): 1478-1488.
[13] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
[14] FAN Genlian, GUO Zhiqi, TAN Zhanqiu, LI Zhiqiang. Architecture Design Strategies and Strengthening-Toughening Mechanisms of Metal Matrix Composites[J]. 金属学报, 2022, 58(11): 1416-1426.
[15] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
No Suggested Reading articles found!