Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (13): 33-38    DOI:
Current Issue | Archive | Adv Search |
DISPERSOID AND SiC PARTICULATE STRENGTHENED Al COMPOSITES Ⅱ. PROPERTIES AND FRACTURE BEHAVIOUR
MA Zongyi;WU Shengjin;LUO Ming;LU Yuxiong;BI Jing(Institute of Metal Researth; Chinese Academy of Scicnces; Shenyang);ZHANG Yuzheng (NorlheasternUniversity; Shenyang)
Cite this article: 

MA Zongyi;WU Shengjin;LUO Ming;LU Yuxiong;BI Jing(Institute of Metal Researth; Chinese Academy of Scicnces; Shenyang);ZHANG Yuzheng (NorlheasternUniversity; Shenyang). DISPERSOID AND SiC PARTICULATE STRENGTHENED Al COMPOSITES Ⅱ. PROPERTIES AND FRACTURE BEHAVIOUR. Acta Metall Sin, 1994, 30(13): 33-38.

Download:  PDF(431KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The tenisle tests and fracture surface analyses on the Al_4C_3. Al_2O_3 dispersoids and SiC particulate strengthened aluminum composites fabricated by mechanical alloying were carried out, as well as elastic modulus and CTE of the composites were measured.It was indicated that the strength of SiC_p/ Al composites is obviously improved due to the formation of Al_4C_3 and Al_2O_3 dispersoids, and increases with increasing C content or oxidation time of aluminum powder. The elevated temperature strength of Al_4C_3 dispersoid and SiC particulate reinforced aluminum composite is superior to that of SiC whisker reinforced 2024Al composite. The elastic modulus of Al_4C_3/ Al composite is raised due to the addition of SiC particulates, and CTE is reduced further.The fracture surfaces of the composites display mixture type of large dimples and fine dimples. The amount of cracked SiC particulates on tensile fracture surfaces of the compsites increases with increasing the strength of compsite matrix.
Key words:  compsite      Al      SiC      Al_4C_3      Al_2O_3      fracture behaviour     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I13/33

1MohnWR,VukolratovichD.JMaterEng,1988;10:2252ArnholdV,BaumgartenJ.PowderMetallInt,1985;17:1683马宗义,吴胜进,宁小光,罗明,吕毓雄,毕敬.金属学报,1994;1:B274MaZY,BiJ,LuYX,LuoM,GaoYX.ScrMetallMater,1993;29:2255BhanuprasadVV,BhatRBV,KuruvillaAK,PrasadKS,PandeyAB,MahajanYR.IntPowderMetall,1991;27:2276BiJ,MaZY,WuSj,LuYX,ShenHW.JMaterSciTechnol,1993;9:617马宗义,毕敬,吕毓雄,申红伟,高荫轩.金属学报,1992;28:B4198MaZY,BiJ,LuYX,LuoM,GaoYXIn:MiraveteAed.,Procof9thIutConfonCompositeMaterials,vol.l,UniversityofZaragoza,WoodheadPublishingLimited,1993:448
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[3] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[4] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[5] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[6] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[7] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[8] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[9] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[10] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[11] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[12] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[13] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[14] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[15] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
No Suggested Reading articles found!