Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (7): 23-27    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF RARE EARTH ON TTT DIAGRAM FOR 0.27C-1Cr STEEL
LU Wei;ZHENG Denghui;XU Zuyao Shanghai Jiao Tong UniversityDepartment of Materials Science;Shanghai JiaoTong University; Shanghai 200030.
Cite this article: 

LU Wei;ZHENG Denghui;XU Zuyao Shanghai Jiao Tong UniversityDepartment of Materials Science;Shanghai JiaoTong University; Shanghai 200030.. INFLUENCE OF RARE EARTH ON TTT DIAGRAM FOR 0.27C-1Cr STEEL. Acta Metall Sin, 1993, 29(7): 23-27.

Download:  PDF(390KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  TTT diagrams of the 0.27C-1Cr and 0.27C-1Cr-RE steels are establishedby means of dilatometric measurement for kinetic curves at different temperatures andmetallographic inspections, and the influence of RE on the TTT diagram is studied. The addi-tion of RE refines austenite grains, retards grain growth rate, raises Ac_3 and makes no changeto Ac_1. The incubation periods for proeutectoid ferrite and bainite are reduced, and the timefor complete transformation for pearlite and bainite are prolonged by the addition of RE. Thecomputation result are in comformity with the experimental ones.
Key words:  Rare earth      TTT diagram      0.27C-1Cr Steel      isothermal transformation     
Received:  18 July 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I7/23

1 Liu He, Zheng Denhui, Xu Zuyao. J Chin Soc Rare Earths. 1992; 10: 189
2 吴承建,张保良,中国稀土学报,1992;10(1) .48.
3 刘宗昌,李承基,兵材料科学与工程,1990;(4) .23.
4 江锡堂,稀土与钢的淬透性,中国机械工程学会材料学会第一届年会论文集,上海,1986,p.351.
5 章复中,稀土在钢铁中的应用,北京:冶金工业出版社.1987,20

6 邱巨峰,稀土在钢铁中的应用,北京:冶金工业出版社.1987,251.
7 徐祖耀,相变原理,北京:科学出版社,1988,176
8 #12
9 Hsu T Y, Mon Yiwen. Acta Metall. 1984; 32: 1469.}
[1] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[2] YANG Tianye, CUI Li, HE Dingyong, HUANG Hui. Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2022, 58(9): 1108-1117.
[3] LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui. Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel[J]. 金属学报, 2022, 58(5): 637-648.
[4] LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie. Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. 金属学报, 2022, 58(3): 365-374.
[5] LIU Zhongwu, HE Jiayi. Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets[J]. 金属学报, 2021, 57(9): 1155-1170.
[6] LU Bin, CHEN Furong, ZHI Jianguo, GENG Ruming. Enhanced Welding Properties of High Strength Steel via Rare Earth Oxide Metallurgy Technology[J]. 金属学报, 2020, 56(9): 1206-1216.
[7] ZHU Jian, ZHANG Zhihao, XIE Jianxin. Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study[J]. 金属学报, 2020, 56(12): 1592-1604.
[8] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[9] Yu HUANG, Guoguang CHENG, You XIE. Modification Mechanism of Cerium on the Inclusions in Drill Steel[J]. 金属学报, 2018, 54(9): 1253-1261.
[10] Xuan YU, Zhihao ZHANG, Jianxin XIE. Microstructure, Ordered Structure and Warm TensileDuctility of Fe-6.5%Si Alloy with Various Ce Content[J]. 金属学报, 2017, 53(8): 927-936.
[11] LIU Zheng, LIU Xiaomei, ZHU Tao, CHEN Qingchun. EFFECTS OF ELECTROMAGNETIC STIRRING WITH LOW CURRENT FREQUENCY ON RE DISTRIBUTION IN SEMISOLID ALUMINUM ALLOY[J]. 金属学报, 2015, 51(3): 272-280.
[12] YAO Zhanquan, ZHAO Zengqi, JIANG Liping,HAO Hongbo, WU Shuangxia,ZHANG Guangrui, YANG Jiandong. EFFECTS OF Ce ADDITION ON THE MICROSTRUCTURE AND MAGNETOSTRICTION OF Fe83Ga17 ALLOY[J]. 金属学报, 2013, 49(1): 87-91.
[13] ZHANG Hui WANG Shaoqing. FIRST-PRINCIPLES STUDY ON THE PHASE STABILITY OF Mg-La AND Mg-Nd BINARY ALLOYS[J]. 金属学报, 2012, 48(7): 889-894.
[14] LIANG Yongchun GUO Jianting; SHENG Liyuan; ZHOU Lanzhang. EFFECTS OF RARE EARTH ELEMENT Gd ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF NiAl-Cr(Mo)-Hf EUTECTIC ALLOY[J]. 金属学报, 2010, 46(5): 528-532.
[15] KONG Gang LIU Renbin LU Jintang CHE Chunshan ZHONG Zheng. STUDY ON GROWTH MECHANISM OF LANTHANUM SALT CONVERSION COATING ON GALVANIZED STEEL[J]. 金属学报, 2010, 46(4): 487-493.
No Suggested Reading articles found!