| PRECIPITATION IN DILUTE Fe-V-N ALLOY |
| ZHANG Hong;Hunan Normal University Shanghai Institute of Metallurgy; Academia SinicaWANG Xiaogang;assoeiate professor.Department of Physies;Hunan Normal University.Changsha 410006 |
|
Cite this article:
ZHANG Hong;Hunan Normal University Shanghai Institute of Metallurgy; Academia SinicaWANG Xiaogang;assoeiate professor.Department of Physies;Hunan Normal University.Changsha 410006. PRECIPITATION IN DILUTE Fe-V-N ALLOY. Acta Metall Sin, 1993, 29(5): 7-10.
|
|
|
Abstract The positron annihilation technique was adopted to study the precipitationprocess in the Fe-V-N alloy. The characteristics of the clustering process of V-N, thebehaviour of V-N-vacancy complex and its influence on the precipitation process are dis-cussed. Over 200℃, quenched V-N-vacancy complex begins to migrate and accelerates theprecipitation. Two stages of precipitation process may be: clustering below 840℃ and growthof flakes over 840℃.
|
|
Received: 18 May 1993
|
1 王小刚,张宏.物理学报,1992;41:1452 2 王小刚,张宏.物理学报,1992;41:1458 3 Jack K H. Heat Treatment'73. London: The Metals Society: 1973: 39 4 Chen T G, Jiang C, Wu Z L. J Phys Colloq, 1985; 46 (C10) : 39 5 江潮.中国科学院上海冶金研究所硕士学位论文,1986 6 罗乐.中国科学院上海冶金研究所博士学位论文,1988 7 Kirkegaard P, Eldrup M. Comput Phys Commun, 1974; 7: 401 8 Mantl S, Friftshauser W. Phys Rev Lett, 1975; 34: 1544 9 Triftshauser W. Phys Rev, 1975; B12: 4634 10 Mackenzie I K, Jackman T E, Lichtenberger P C. Appl Phys, 1976; 9: 259 11 Luhr-Tanck W, Ederhof M, Sager A, Bosse H. Mater Sci Forum, 1987: 15--18: 629 12 王小刚.中国科学院上海冶金研究所博士学位论文,1990F |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|