| EFFECT OF Ti ON MICROSTRUCTURE OF STEEL 321 FILM SYNTHESIZED BY MAGNETRON SPUTTERING DEPOSITION |
| YANG Dejun;ZHOU Honghui;LI Huiqin University of Science and Technology Beijing professor;Department of Corrosion Engineering; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
YANG Dejun;ZHOU Honghui;LI Huiqin University of Science and Technology Beijing professor;Department of Corrosion Engineering; University of Science and Technology Beijing; Beijing 100083. EFFECT OF Ti ON MICROSTRUCTURE OF STEEL 321 FILM SYNTHESIZED BY MAGNETRON SPUTTERING DEPOSITION. Acta Metall Sin, 1993, 29(4): 81-84.
|
|
|
Abstract Effect of increasing content of Ti on the crystalline to amorphous transition inalloy films of stainless steel 321 plus Ti synthesized by high rate magnetron sputtering deposi-tion is reported. X-ray diffraction analysis revealed that the microstructure of film issequently changed from α-Fe, α-Fe+x-phase, microcrystalline-amorphous into amorphouswith increasing content of Ti from 0-3, 3-10, 10-18 to 18-30wt-% respectively.
|
|
Received: 18 April 1993
|
1 单大勇.北京科技大学硕士学位论文,1989 2 Dahlgren S D. Metall Trans, 1970; 1: 2095 3 Andrews K W. Nature, 1949: 164: 1015 4 Hughes H, Llewelyn, D. J Iron Steel Inst, 1959; 192: 170 5 Brimhall J L. Charlot L A, Kissinger H E. J Mater Sci, 1982; 17: 1149 6 王一禾,杨膺善主编,非晶态合金,北京:冶金工业出版社,1989 7 戴道生,韩汝琪编.非晶态物理.北京:电子工业出版社,1989 8 Wang Rong. In: Bennett L ed., Theory of Alloy Phase Formation, New York: AIME, 1980: P472 9 Wang Rong, J Mater Sci, 1982; 17: 1142 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|