LI Xiaogang;CHEN Huan;YAO Zhiming;LI Jin;KE Wei Institute of Corresion and Protection of Metals; Academia Sinica; Shenyang lecturer;Institute of Corrosion and Protection of Metals;Academia Sinica; Shenyang 110015. HYDROGEN ATTACK ON AUSTENITIC STEEL 304 UNDER HIGH TEMPERATURE AND HIGH PRESSURE. Acta Metall Sin, 1993, 29(4): 73-76.
|
|
|
Abstract Hydrogen attack on 304 austenitic stainless steel in the service for 2×10~4 h at450℃ under 5 MPa was detected to result from the occurrence of Cr_(23)C_6. The methane bub-bles were formed preferentially along grain boundaries and twin boundaries, and some ofthem in grains. Experimental results and thermodynamical analysis indicated that the Cr-de-pleted region around bubbles is not necessary condition in growth stage of bubbles.
|
|
Received: 18 April 1993
|
1 Inglis N P, Andrews W J. J Iron Steel Inst. 1933, 128: 383 2 Dodge S, Barnett F, Trans ASME, 1953; 75: 331 3 Nelson G A, Werkst Korros, 1963; 14: 65 4 Yacaman M J, Parthasarathy T A, Hirth J P. Metall Trans, 1984; 15A: 1485. 5 Dilewijns J, Houkaert Y. Proceedings of the International Conference on Interaction of Steels with Hydrogen in Petroleum Industry Pressure Vessel Service, Materials Properties Cocencil, Paris, 1989: 167 6 Kubaschewski O, Alcock C B. Metal Thermochemistry. Oxford: Pergamon, 1979: 300 7 Odette G R, Vagarali S S, Metall Trans, 1982; 13A: 299 8 Sundararajan G, Shewmon P G. Metall Trans, 1980; 11A: 509 9 Lopez H, Shewmon P G. Acta Metall. 1983; 31: 1945/ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|