Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (4): 68-72    DOI:
Current Issue | Archive | Adv Search |
HOT CORROSION OF THREE M_3Al-TYPE INTERMETALLICS AT 600℃
NIU Yan;WU Weitao;GESMUNDO F;VIANI F;Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academai Sinica; Shenyang; Instituta di Chimica; Facolta di Ingegneria; Universita di Genova Research associate;Institute of Corrosion and Protection of Metals;Academia Sinica; Shenyang 110015
Cite this article: 

NIU Yan;WU Weitao;GESMUNDO F;VIANI F;Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academai Sinica; Shenyang; Instituta di Chimica; Facolta di Ingegneria; Universita di Genova Research associate;Institute of Corrosion and Protection of Metals;Academia Sinica; Shenyang 110015. HOT CORROSION OF THREE M_3Al-TYPE INTERMETALLICS AT 600℃. Acta Metall Sin, 1993, 29(4): 68-72.

Download:  PDF(1034KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Na_2SO_4 deposits accelerate significantly the corrosion rates of 3 intermetallicsFe_3Al, Ni_3Al and Ti_3Al in the simulated combustion gases at 600℃. The corrosion product ismixture of oxides and sulphides of both the base metal and Al. Corrosion resistance of Fe_3Aland Ti_3Al is superior to that of Ni_3Al owing to the formation of an inner layer rich inAl_2O_3 for Fe_3Al and of an intermediate layer composed of TiO_2 and NbO_2 for Ti_3Al modi-fied by Nb. While, Ni_3Al forms an inner layer which is so abundant in Ni sulphide as to facili-tate the migration of Ni outward. The addition of NaCl to Na_2SO_4 has no significant influ-ence on the corrosion behaviour of the three intermetallics.
Key words:  hot corrosion      intermetallic      aluminide      M_3Al     
Received:  18 April 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I4/68

1 Strirger J. Mater Sci and Technol, 1987; 3: 482
2 Rapp R A. J Mater Sci Eng, 1987; 87: 319
3 Meier G H. In: Grobstein T, Doychak J eds., Oxidation of High-Temperature Intermetallics, Wamendale: TMS, PA, 1989: 1
4 Niu Y, Wu W, Guo J, Zhang Y. In: Zhu R Z et.al. eds., Corrosion Control, Proc 7th Asian-Pacitic Corrosion Control Conference, Vol. 1, Beijing: Intern Academic, 1990: 130
5 Zhen C, Zhang J, Niu Y, Wu W, Presented at the 12th Internatioal Symposion on Reacfivity of Solids, September 29--30, 1992, Madrid (spain)
6 Shi L, Zang Y, Shih S. In: Zhu R Z et. al. eds., Corrosion Control, Proc 7th Asian-Pacitic Corrosion Control Conference, Vol. 1, Beijing: Intern Academic, 1990: 42
7 Zhang Y, Shih S, Cao T. In: Zhu R Z et. al. eds., Corrosion Control, Proc 7th Asian-Pacitic Corrosion Control Conference, Vol. 1, Beijing: Intern Academic, 1990: 124
8 Rapp R A. In: Johannesen O, Awdersen A G eds., Selected Topics in High Temperature Chemistry. Amsterdam: Elsevier, 1989: 129
9 Gesmundo F, Young D J, Roy S K. High Temp Mater Proc, 1989; 8: 149
[1] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[2] ZHOU Lijun, WEI Song, GUO Jingdong, SUN Fangyuan, WANG Xinwei, TANG Dawei. Investigations on the Thermal Conductivity of Micro-Scale Cu-Sn Intermetallic Compounds Using Femtosecond Laser Time-Domain Thermoreflectance System[J]. 金属学报, 2022, 58(12): 1645-1654.
[3] WANG Di, WANG Dong, XIE Guang, WANG Li, DONG Jiasheng, CHEN Lijia. Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy[J]. 金属学报, 2021, 57(6): 780-790.
[4] GONG Shengkai, SHANG Yong, ZHANG Ji, GUO Xiping, LIN Junpin, ZHAO Xihong. Application and Research of Typical Intermetallics-Based High Temperature Structural Materials in China[J]. 金属学报, 2019, 55(9): 1067-1076.
[5] Hua JI,Yunlai DENG,Hongyong XU,Weiqiang GUO,Jianfeng DENG,Shitong FAN. The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z[J]. 金属学报, 2019, 55(3): 376-388.
[6] Liqun CHEN, Zhengchen QIU, Tao YU. Effect of Ru on the Electronic Structure of the [100](010) Edge Dislocation in NiAl[J]. 金属学报, 2019, 55(2): 223-228.
[7] Yimin LIAO, Min FENG, Minghui CHEN, Zhe GENG, Yang LIU, Fuhui WANG, Shenglong ZHU. Comparative Study of Hot Corrosion Behavior of theEnamel Based Composite Coatings and the ArcIon Plating NiCrAlY on TiAl Alloy[J]. 金属学报, 2019, 55(2): 229-237.
[8] CAO Lihua, CHEN Yinbo, SHI Qiyuan, YUAN Jie, LIU Zhiquan. Effects of Alloy Elements on the Interfacial Microstructure and Shear Strength of Sn-Ag-Cu Solder[J]. 金属学报, 2019, 55(12): 1606-1614.
[9] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[10] HE Xianmei, TONG Liuniu, GAO Cheng, WANG Yichao. Effect of Nd Content on the Structure and Magnetic Properties of Si(111)/Cr/Nd-Co/Cr Thin Films Prepared by Magnetron Sputtering[J]. 金属学报, 2019, 55(10): 1349-1358.
[11] Min ZHANG, Erlong MU, Xiaowei WANG, Ting HAN, Hailong LUO. Microstructure and Mechanical Property of the Welding Joint of TA1/Cu/ X65 Trimetallic Sheets[J]. 金属学报, 2018, 54(7): 1068-1076.
[12] Huijun KANG, Jinling LI, Tongmin WANG, Jingjie GUO. Growth Behavior of Primary Intermetallic Phases and Mechanical Properties for Directionally Solidified Al-Mn-Be Alloy[J]. 金属学报, 2018, 54(5): 809-823.
[13] Chengyang JIANG, Yingfei YANG, Zhengyi ZHANG, Zebin BAO, Shenglong ZHU, Fuhui WANG. Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating[J]. 金属学报, 2018, 54(4): 581-590.
[14] Lin GENG, Hao WU, Xiping CUI, Guohua FAN. Recent Progress on the Fabrication of TiAl-Based Composites Sheet by Reaction Annealingof Elemental Foils[J]. 金属学报, 2018, 54(11): 1625-1636.
[15] Xuan YU, Zhihao ZHANG, Jianxin XIE. Microstructure, Ordered Structure and Warm TensileDuctility of Fe-6.5%Si Alloy with Various Ce Content[J]. 金属学报, 2017, 53(8): 927-936.
No Suggested Reading articles found!