| EFFECT OF MISCHMETAL ON REACTION BETWEEN SOLID IRON AND LIQUID Zn+5wt-%Al ALLOY |
| YANG Yun;YU Zongsen University of Science and Technology Beijing |
|
Cite this article:
YANG Yun;YU Zongsen University of Science and Technology Beijing. EFFECT OF MISCHMETAL ON REACTION BETWEEN SOLID IRON AND LIQUID Zn+5wt-%Al ALLOY. Acta Metall Sin, 1993, 29(12): 14-20.
|
|
|
Abstract Effect of mischmetal on the reaction between iron panels and Zn+5wt-%Alliquid alloy during hot dipping at 450℃ was investigated. After about 2--4s interval, anintermetallic layer may form and grow, and it will be postponed to 64-128s if themischmetal added in liquid alloy bath. The structure of the intermetallic layer has been stu-died by SEM, EDX, XRD, EMPA and TEM. The AES record in depth analysis shows thatthe rare earth elements segregated at the interface between iron panel and liquidZn+5wt-% Al alloy. The effect of mischmetal addition was discussed.
|
|
|
1 Goddwin F E. Proc of the 14th Int Galvanizing Conf, Munich, Germany, London: ZOA, 1985: Ⅱ 2 Skenazi A F. Proc of the 14th Int Galvanizing Conf, Munich, Germany, London: ZOA, 1985: OA/1 3 Li Y Z, Liu C, Lu J T, Chen J H. Proc Int Conf on Zinc and Zinc Alloy Coated Steel Sheet, Tokyo, Japan, 1989: 374 4 Pelerin J, Serrais J P, Contsouradis D, Herrschaft D C, Radtke S F. Proc 13th Int Galvanizing Conf, London: ZOA, 1982: 49/1 5 Urednicok M, Kiraldy J S. Metall Trans, 1970; 2: 2903 6 Caceres P G, Hotham C A, Spittle J A, Jones R D. Mater Sci Technol, 1986; 2: 871 7 Chen Z W, Sharp R M, Gregory J T. Mater Sci Technol, 1990; 6: 1173 8 Chen Z W, Gregory J T, Sharp R M. CASS90: Corrosion-Air, Sea, Soil (Proc Conf), Auckland, New Zealand, 1990: 19 9 Selverian J H, Marder A R, Notis M R. Metall Trans, 1988; 19A: 1193 10 Lamkov L N. Avtom Svarka, 1971; (6) : 64 11 Lamkov L N, Falchenko V M, Polishchuk D F, Ryaboranda V R, Lozovskuya V. Prot Coat Met, 1970; 3: 66 12 Heumann V T, Dittrich D. Z Metallk, 1959; 50: 617 13 Black P J. Acta Cryst allogr, 1955; 8: 175 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|