| EFFECT OF NITROGEN ON GRAPHITE MORPHOLOGY IN GRAY CAST IRON |
| ZHAI Qijie; HU Hanqi (University of Science and Technology Beijing) |
|
Cite this article:
ZHAI Qijie; HU Hanqi (University of Science and Technology Beijing). EFFECT OF NITROGEN ON GRAPHITE MORPHOLOGY IN GRAY CAST IRON. Acta Metall Sin, 1992, 28(10): 73-78.
|
|
|
Abstract The distribution of nitrogen and morphology of graphite in the gray cast iron containing nitrogen were studied by adopting the man-made specimens of Fe-C-Si-Mn alloys with some nitrogen added. The nitrogen adsorbed along interfaces between graphite and matrix together with solid-solutioned in graphite is believed to be the principal cause of morphological variation of graphite.
|
|