| MECHANISM OF DEUTERIUM CRACKING IN PALLADIUM |
| SUN Dalin; LEI Yongquan; CHEN Yanglin; WU Jing; WANG Qidong (Zhejiang University; Hangzhou) |
|
Cite this article:
SUN Dalin; LEI Yongquan; CHEN Yanglin; WU Jing; WANG Qidong (Zhejiang University; Hangzhou). MECHANISM OF DEUTERIUM CRACKING IN PALLADIUM. Acta Metall Sin, 1992, 28(10): 36-40.
|
|
|
Abstract After 290 h electrochemically deuterium charged, the density of dislocations in well-annealled Pd increased from 10~8/cm~2 to 10~(12)/cm~2 above, and a large amount of bubble-like structure or cracks have been observed by optical and transmission electronic microscopes. The mechanism of deuterium cracking was considered to be the formation of D_2 due to the segregation and recombination of deuterium atoms around dislocations. XRD results showed that the lattice constant of Pd increased from 0.3890 to 0.4034 nm.
|
|
Received: 18 October 1992
|
1 Fast J D. Gases in Metals. London: Philips, 1976: 85 2 耿东升,谢利卿,李烈风.理化检验(物理分册),1990;26(2) :26 3 孙大林.浙江大学博士学位论文,1991 4 Brodowsky H. Z Phys Chem, Neue Folge, 1965; 44: 129 5 褚武杨.氢损伤和滞后断裂.北京:冶金工业出版社,1988:14 6 Verhoeven J D. Fundamentals of Physical Metallurgy. New York: Wiley, 1975: 106 7 李振寰.元素性质数据手册.石家庄:河北人民出版社,1980:76 8 张万箱.冷核聚变学术交流与对策研讨会,北京,1990 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|