FINE STRUCTURE ANALYSIS OF DEFORMED AUSTENITE STAINLESS STEEL 1Cr18Ni9
TENG Feng'en;WANG Yuming;XU Yue Jilin University; Chang chun
Cite this article: 

TENG Feng'en;WANG Yuming;XU Yue Jilin University; Chang chun. FINE STRUCTURE ANALYSIS OF DEFORMED AUSTENITE STAINLESS STEEL 1Cr18Ni9. Acta Metall Sin, 1992, 28(1): 45-47.

Download:  PDF(606KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The intensity distribution curves for austenite stainless steel 1Cr18Ni9 after 1080℃ W. Q. and de-formed under uniaxial tension at different degrees of strain have been examined by step scanning X--ray diffraction technique. The effective domain size, dislocation density inside domains, dislocation istrubutionparameter, density of stored energy, etc. were obtained by profile analysis. In comparison with TEM observation,the grain is similar in size to subgrain, but the minimum width of stacking faults differs with the characteristic one, which may be related to the variation of stacking fault width
Key words:  austenite stainless steel      fine structure      X-ray analysis     
Received:  18 January 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I1/45

1 桑野三郎.材料,1977;26(287) :735--741
2 Nair PK, Vasudevan R. J Appl Crystallogr, 1977; 10: 401--404
3 滕凤恩,王煜明.理化检验(物理分册),1989;(2) :40--49
4 滕凤恩,崔相旭.物理学报,1989;38:1845--1848
5 Tung Feng-en (Teng Feng'en), Wang Yuming. J Mater Sci, 1986; 21: 3223--3226*
[1] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[2] PENG Yun,SONG Liang,ZHAO Lin,MA Chengyong,ZHAO Haiyan,TIAN Zhiling. Research Status of Weldability of Advanced Steel[J]. 金属学报, 2020, 56(4): 601-618.
[3] Dawei WANG,Shichao XIU. Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint[J]. 金属学报, 2017, 53(5): 567-574.
[4] Xiaosong ZHANG,Yong XU,Shihong ZHANG,Ming CHENG,Yonghao ZHAO,Qiaosheng TANG,Yuexia DING. Research on the Collaborative Effect of Plastic Deformation and Solution Treatment in the Intergranular Corrosion Property of Austenite Stainless Steel[J]. 金属学报, 2017, 53(3): 335-344.
[5] YANG Hui, XIA Shuang, ZHANG Zilong, ZHAO Qing, LIU Tingguang, ZHOU Bangxin, BAI Qin. IMPROVING THE INTERGRANULAR CORROSION RESISTANCE OF THE WELD HEAT-AFFECTED ZONE BY GRAIN BOUNDARY ENGINEERING IN 304 AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(3): 333-340.
[6] HUANG Hefei, LI Jianjian, LIU Renduo, CHEN Huaican, YAN Long. TEMPERATURE EFFECT OF Xe ION IRRADIATION TO 316 AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2014, 50(10): 1189-1194.
[7] ZHANG Weihu ZHANG Fuchun ZHANG Zhiyong YAN Junfeng . FIRST–PRINCIPLE ANALYSYS ON FINE STRUCTURE OF Pb0.5Sr0.5TiO3[J]. 金属学报, 2009, 45(2): 217-222.
[8] DONG Dan-Yang; Changsheng LIU. INVESTIGATION OF HYPERFINE STRUCTURE OF LASER CLADDING Fe-Si COATING[J]. 金属学报, 2008, 44(2): 188-192 .
[9] LUO Chengping(C.P.Luo);LIU Jiangwen;XIAO Xiaoling(Department of Mechanical Engineering; South China University of Technology; Guangzhou 510641)Correspondent:LUO Chengping; professor; Tel:(020)85511617; Fax: (020)87111312;E-mail: mecpluo@letterbox.scut.edu.cn. FINE STRUCTURE AND CRYSTALLOGRAPHY OF ISOTHERMAL LOWER BAINITE IN AN EXPERIMENTAL STEEL 38Si2Mn2Mo[J]. 金属学报, 1998, 34(10): 1009-1015.
[10] LI Fengzhao; AO Qing; GU Yingni; JIANG Jiang; SUN Dongsheng (Shandong University of Technology; Jinan 250061)DAI Jiyan; PENG Hongying (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015). TEM OBSERVATION OF THE FINE STRUCTURE OF BAINITE[J]. 金属学报, 1997, 33(3): 241-247.
[11] FANG Hongsheng; YANG Zhigang; WANG Jiajun; ZHENG Yankang(Tsinghua University; Beijing 100084)(Manuscript received 1995-11-10). RESEARCH ASPECTS OF TRANSFORMATION AND APPLICATION OF BAINITE AND MARTENSITE[J]. 金属学报, 1996, 32(4): 337-350.
[12] LI Douxing; PING Dehai; NING Xiaoguang; YE Hengqiang (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; Shenyang). FINE STRUCTURE OF BOTH INTERFACES AND INTERFACIAL REACTION PRODUCTS[J]. 金属学报, 1992, 28(7): 1-18.
[13] LI Delin; YANG Gencang; ZHOU Yaohe (Northwestern Polytechnical University; Xi'an). RECALESCENCE AND SOLIDIFICATION MICROSTRUCTURE OF HIGHLY UNDERCOOLED ALLOY Ni_(68)B_(21)Si_(11).[J]. 金属学报, 1992, 28(10): 1-5.
[14] XU Yourong;GU Qing;WANG Deying Shanghai University of Science and Technology; GU Jufang;QU Tiancai Shanghai Iron and Steel Research Institute. DYNAMIC MECHANICAL BEHAVIOURS OF HIGH Mo AUSTENITE STAINLESS STEEL DURING HOT DEFORMATION[J]. 金属学报, 1991, 27(4): 134-138.
[15] ZHU Min;LI Cuobin YANG Dazhi Dalian University of Technology Department of Materials Engineering; Dailian University of Technology; Dailian 116024. FINE STRUCTURE VARIATION OF POLYCRYSTALLINE Cu-Zn-Al SHAPE MEMORY ALLOY UNDER MARTENSITE DEFORMATION[J]. 金属学报, 1990, 26(1): 72-75.
No Suggested Reading articles found!