EFFECT OF HEAT TREATMENT ON CRACK PROPAGATING RATE OF GC-4 STEEL FROM CORROSION FATIGUE OR STRESS CORROSION IN VARIOUS MEDIA
LU Minxu;LIU Xiaokun;WANG Jianjun;FU Xiangjiong;ZHENG Xiulin Northwestern Polytechnical University; Xi'an
Cite this article: 

LU Minxu;LIU Xiaokun;WANG Jianjun;FU Xiangjiong;ZHENG Xiulin Northwestern Polytechnical University; Xi'an. EFFECT OF HEAT TREATMENT ON CRACK PROPAGATING RATE OF GC-4 STEEL FROM CORROSION FATIGUE OR STRESS CORROSION IN VARIOUS MEDIA. Acta Metall Sin, 1991, 27(6): 115-121.

Download:  PDF(610KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Comparative investigations were ca1ricd cut of tLe efItct of Leat 1reatment regimes for GC--4 steel, 40CrMnSiMoVA, on its c1ack p1opagating ratcs, from corrosion fatigue, (da/dN)..' or stress cor1osion crackirg, (do/dt),.,', in mcdia with various constituents and VH va1ues. Both (da/dN).. 8'r d (do/dt),.. acce!cra1e wi1h tbe increase of yieId stress of the steel, yet the fOraner js far 1ess tLan 1Le l8tcr. ]n ccmparison with mcdia, tLe (do/dt),,. in distil1td water is sligLt1y grca1cr 1Lan tbat in 3.5% NaCl solution, and tLe (dQ/dN)., in distil1cd water is far less ttan tkat in 3.5% NaCl solution. With the pH value increasing in 3.5% NLCl ao1ution, 1le (do/dN). F lQwerS down and the (da/dt),.. specds up. An xplahation was a1Eo r1oroltd witb concept of the cyclic bardening and softeniDg at crack tip, as we1l as the crack c1osure and occluded ceU effect.
Key words:  crack propagating rate      corrosion fatigue      stress corrosion cracking      heat treatment      pH value     
Received:  18 June 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I6/115

1 郑文龙,朱国培,欧阳怀谨,李革.金属学报,1986;22:A275--A282
2 陈汉存、刘正义,庄育智.中国腐蚀与防护学报,1989;9(2) :79--86
3 郑文龙,蔡安定,朱国培.金属学报,1983;19:A134--A141
4 路民旭,王建军,刘晓坤,郑修麟.航空学报,1990;11:B617--B621
5 王建军,刘晓坤,路民旭.航空学报,1988;9(13) :S140--S143
6 林栋梁,吴建生,杨正瑞.金属学报,1983;19:A165--A167
7 Gerberich W W. In: Bernstein I M, Thompson A W eds., Hydrogen in Metals, ASM, 1974: 115
8 陈大明,康沫狂,谭若兵.西北工业大学学报,1990;(Suppl.):188--196
9 Turnbull A. Br Corros J, 1980; 15: 162--171
10 Sandoz G. In: Brown B F ed, Stress-Corrosion Cracking in High Strength Steels and in Titanium and Aluminium Alloy, Chapter 3: High Strength Steel, Washington D C.: Naval Research Laboratory, 1972: 79--146
11 Turnbull A, Ferriss D H. Corros Sci, 1987; 27: 1323--1350
[1] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[2] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[3] YANG Lei, ZHAO Fan, JIANG Lei, XIE Jianxin. Development of Composition and Heat Treatment Process of 2000 MPa Grade Spring Steels Assisted by Machine Learning[J]. 金属学报, 2023, 59(11): 1499-1512.
[4] SUN Tengteng, WANG Hongze, WU Yi, WANG Mingliang, WANG Haowei. Effect ofIn Situ 2%TiB2 Particles on Microstructure and Mechanical Properties of 2024Al Additive Manufacturing Alloy[J]. 金属学报, 2023, 59(1): 169-179.
[5] HAN Linzhi, MU Juan, ZHOU Yongkang, ZHU Zhengwang, ZHANG Haifeng. Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy[J]. 金属学报, 2022, 58(9): 1159-1168.
[6] LI Zhao, JIANG He, WANG Tao, FU Shuhong, ZHANG Yong. Microstructure Evolution of GH2909 Low Expansion Superalloy During Heat Treatment[J]. 金属学报, 2022, 58(9): 1179-1188.
[7] MA Zhimin, DENG Yunlai, LIU Jia, LIU Shengdan, LIU Honglei. Effect of Quenching Rate on Stress Corrosion Cracking Susceptibility of 7136 Aluminum Alloy[J]. 金属学报, 2022, 58(9): 1118-1128.
[8] ZHANG Jiarong, LI Yanfen, WANG Guangquan, BAO Feiyang, RUI Xiang, SHI Quanqiang, YAN Wei, SHAN Yiyin, YANG Ke. Effects of Heat Treatment on Microstructure and Mechanical Properties of a Bimodal Grain Ultra-Low Carbon 9Cr-ODS Steel[J]. 金属学报, 2022, 58(5): 623-636.
[9] ZENG Xiaoqin, WANG Jie, YING Tao, DING Wenjiang. Recent Progress on Thermal Conductivity of Magnesium and Its Alloys[J]. 金属学报, 2022, 58(4): 400-411.
[10] YUAN Bo, GUO Mingxing, HAN Shaojie, ZHANG Jishan, ZHUANG Linzhong. Effect of 3%Zn Addition on the Non-Isothermal Precipitation Behaviors of Al-Mg-Si-Cu Alloys[J]. 金属学报, 2022, 58(3): 345-354.
[11] CHEN Run, WANG Shuai, AN Qi, ZHANG Rui, LIU Wenqi, HUANG Lujun, GENG Lin. Effect of Hot Extrusion and Heat Treatment on the Microstructure and Tensile Properties of Network Structured TiBw/TC18 Composites[J]. 金属学报, 2022, 58(11): 1478-1488.
[12] WANG Di, HUANG Jinhui, TAN Chaolin, YANG Yongqiang. Review on Effects of Cyclic Thermal Input on Microstructure and Property of Materials in Laser Additive Manufacturing[J]. 金属学报, 2022, 58(10): 1221-1235.
[13] WANG Wenquan, WANG Suyu, CHEN Fei, ZHANG Xinge, XU Yuxin. Microstructure and Mechanical Properties of TiN/Inconel 718 Composites Fabricated by Selective Laser Melting[J]. 金属学报, 2021, 57(8): 1017-1026.
[14] WANG Yue, WANG Jijie, ZHANG Hao, ZHAO Hongbo, NI Dingrui, XIAO Bolv, MA Zongyi. Effects of Heat Treatments on Microstructure and Mechanical Properties of AlSi10Mg Alloy Produced by Selective Laser Melting[J]. 金属学报, 2021, 57(5): 613-622.
[15] TAN Jibo, WANG Xiang, WU Xinqiang, HAN En-Hou. Corrosion Fatigue Behavior of 316LN Stainless Steel Hollow Specimen in High-Temperature Pressurized Water[J]. 金属学报, 2021, 57(3): 309-316.
No Suggested Reading articles found!