Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (5): 54-60    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF MICROSTRUCTURE OF ALUMINIDE COATING ON HIGH-CYCLE FATIGUE PERFORMANCE OF COATING-SUPERALLOY SYSTEM
FAN Ruilin Institute of Aeronautical Materials; Beijing
Cite this article: 

FAN Ruilin Institute of Aeronautical Materials; Beijing. EFFECT OF MICROSTRUCTURE OF ALUMINIDE COATING ON HIGH-CYCLE FATIGUE PERFORMANCE OF COATING-SUPERALLOY SYSTEM. Acta Metall Sin, 1991, 27(5): 54-60.

Download:  PDF(1677KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The high-cycle fatigue performance of different microstructures of aluminide coating-superalloy system has been studied at 900℃. The single phase coating of coarse equiaxial grain NiAl (β) has unfavourabie effect on fatigue life of the coating-superalloy. The fatigue life may shorten if the coating of NiAl (β) was an enrichment of coarse refractory metal grains. While an improvement can be made by dispersing numerous secondary phase particles such as extreme fine γ', quasi-σ phase and others.
Key words:  aluminide coating      coating microstructure      high temperature      high cycle fatigue     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/54

1 Strang A. In: Kirman I, Marriott J B, Merz M, Sahm P R, Whittle D P eds., Behaviour of High Temperature Alloys in Aggressive Environments, London: The Metals Society, 1980: 595--613
2 Paskiet G F, Boone D H, Sullivan C P. J Inst Met (London), 1972; 100: 58--62
3 Wells C H, Sullivan C P. ASM Trans Q, 1968; 61: 149--155
4 Goward G W, Boone D H. Oxid Met, 1971; 3: 475--495
5 Goward G W, Boone D H, Giggins C S. ASM Trans Q, 1967; 60. 228--241
6 Levine S R, Caves R M. J Electrochem Soc, 1974; 121: 1051--1064
7 Pichoir R. In: Holmes D R, Rahmel A eds., Materials and Coation to Resist High Temperature Corrosion. London: Applied Science. 1978: 253--269
8 杨炳光,李永祚,范瑞麟,杨树梅.中国腐蚀与防护学报,1985;5:142-14
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[3] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[4] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[5] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[6] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[7] XU Jinghui, LI Longfei, LIU Xingang, LI Hui, FENG Qiang. Thermal-Stress Coupling Effect on Microstructure Evolution of a Fourth-Generation Nickel-Based Single-Crystal Superalloy at 1100oC[J]. 金属学报, 2021, 57(2): 205-214.
[8] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[9] LI Xiaohui, WANG Jianqiu, HAN En-Hou, GUO Yanjun, ZHENG Hui, YANG Shuangliang. Electrochemistry and In Situ Scratch Behavior of 690 Alloy in Simulated Nuclear Power High Temperature High Pressure Water[J]. 金属学报, 2020, 56(11): 1474-1484.
[10] BAO Feiyang, LI Yanfen, WANG Guangquan, ZHANG Jiarong, YAN Wei, SHI Quanqiang, SHAN Yiyin, YANG Ke, XU Bin, SONG Danrong, YAN Mingyu, WEI Xuedong. Corrosion Behaviors and Mechanisms of ODS Steel Exposed to Static Pb-Bi Eutectic at 600 and 700 ℃[J]. 金属学报, 2020, 56(10): 1366-1376.
[11] LI Jiarong,XIE Hongji,HAN Mei,LIU Shizhong. High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1195-1203.
[12] Jinyao MA,Jin WANG,Yunsong ZHAO,Jian ZHANG,Yuefei ZHANG,Jixue LI,Ze ZHANG. Investigation of In Situ 1150 ℃ High Temperature Deformation Behavior and Fracture Mechanism of a Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(8): 987-996.
[13] Zhengkai WU, Shengchuan WU, Jie ZHANG, Zhe SONG, Yanan HU, Guozheng KANG, Haiou ZHANG. Defect Induced Fatigue Behaviors of Selective Laser Melted Ti-6Al-4V via Synchrotron Radiation X-Ray Tomography[J]. 金属学报, 2019, 55(7): 811-820.
[14] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[15] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
No Suggested Reading articles found!