Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (5): 106-109    DOI:
Current Issue | Archive | Adv Search |
DISTRIBUTION OF MICROHARDNESS ALONG INTERFACE OF (N~++IP)-TiN COMPOSITE COATING ON STEEL
JIN Zhujing;YU Li;YU Zhiming;DAI Shaoxia;XU Jiayin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang Corrosion Science Laboratory Academia Sinica
Cite this article: 

JIN Zhujing;YU Li;YU Zhiming;DAI Shaoxia;XU Jiayin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang Corrosion Science Laboratory Academia Sinica. DISTRIBUTION OF MICROHARDNESS ALONG INTERFACE OF (N~++IP)-TiN COMPOSITE COATING ON STEEL. Acta Metall Sin, 1991, 27(5): 106-109.

Download:  PDF(605KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The composite coating of (N~++IP)-TiN was prepared by ion-plated TiN film onto ion-nitrided case on the low carbon steel substrate. The microhardness measurement along interface between IP-TiN coating and substrate was detected as a moderate decrease in magnitude with increase of distance from the coating surface.This seems due to the occurrence of ion nitride case, ε-Fe_3N-Fe_2N and Fe_4N phases, along the interface.
Key words:  microhardness      composite coating      inierface      ion-plating      ion     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/106

1 金柱京,于力,戴少侠,于志明.金属学报,1989;25:B55
2 刘长清,于志明,金柱京,于力,徐家寅.中国稀土学报,待发表
3 Eckertova L,王广阳,张福初,梁民基译.薄膜物理学.北京;科学出版社,1986:157-159
4 Rickerby D S, Burnett P J. Thin Solid Films, 1988; 157: 195--222
5 Jacobson B E, Nimmagadda R, Bunshah R F. Thin Solid Films, 1979; 63: 333
6 Benjamin P, Weaver C. Proc R Soc, London, ser. A, 1960; 254: 163
7 胡倾宇.中国科学院金属研究所硕士论文,1986
8 金柱京,于力,戴少侠,于志明.金属学报,1990;26:B16
9 东北工学院材料系编.金属材料及热处理.沈阳:东北工学院,1976:355-381S
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[4] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[5] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[6] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[7] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[8] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[9] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[10] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[11] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[12] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[13] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[14] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[15] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
No Suggested Reading articles found!